The Luristan Project - Large Pictures of Cut Sword

These very large picture serve as permanent record of the project results. Some experts may recognize features not evident to us.
The first picture shows the positions of the scan once more for convenience
   
Part of Kiel half; polished and Nital etched.
Strongly contrast enhanced.
   
Scan through the backside of the left head (animal part; 1 - 14). Turned 90o for convenience
 
Luristan mask sword project
Link to text
 
Scan through the backside of the right head (animal part; (15 - 26) and the "bead" region (38 - 27) Turned 90o for convenience
   
.
Link to the text
     
Scan through the hilt at the upper ring position (97 - 120)
 
Link to text
   
Scan through the hilt at the middle ring position (152 - 183)
 
Link to text
   
Scan through the hilt at the bottom ring position (121 - 151)
 
Link to text
   
Scan through the animals and the hilt (39 - 77)
 
Link to text
     
Scan through the blade close to the hilt (upper blade; 184 - 190)
 
Link to text
   
Scan through the blade in the middle (middle blade; Nital 191 - 196; Oberhoffer 275 - 281):
 
 
Link to text
     
Scan through the bottom end of the blade (197 - 202)
Link to text
     

With frame With frame as PDF

go to Sword Types

go to Discussion of the "Cut Sword" Findings

go to Faggoting

go to Sword Places: Luristan

go to Banding

go to Etching Steel

go to More Luristan Swords

go to Large Pictures - Chapter 11.1

go to Luristan Special

go to The Luristan Project - Results from Cut Swords

go to The Luristan Project - Results from Cut Swords Part 2

go to The Luristan Project - Results from Cut Swords

go to Luristan Project - Large Pictures

© H. Föll (Iron, Steel and Swords script)