Exercise 2.1-1 Free Electron Gas with Constant Boundary Conditions

Consider the free electron gas model but let the boundary conditions be: y(0) = y(L) = 0, i.e. we have fixed boundary conditions.
Derive the solution to the Schrödingerequation and the density of states for this case.
Show that the number of states is the same as for the periodic boundary conditions as given in the backbone
 
 

Link to the solution