Thermodynamics of Point Defects in Ionic Crystals described by Mass Action Law    
Explain the extension of the mass actio law to defects. Discuss shortly the problems with notation (Schottky, Kröger-Vink)    
Give a simple example for the application to ionic crystals    
Give a more complex example involving Brouwer diagrams    
All necessary information can be found in the hyperscript.    
Point defects in iron and steel    
Present and discuss the available data for vacancies and self interstitial in bcc and fcc iron (ferrite and austenite).    
Discuss the influence of magnetization on diffusion.    
Present and discuss the available data for carbon interstitials in bcc and fcc iron (ferrite and austenite).    
Consequences for the processing of steel.    
Dislocations and Plastic Deformation in Hexagonal Crystals


Describe the specialities of plastic deformation in hex. crystals as a function of the crystal and defect symmetry    
Give examples, discuss the technical importance.    
Dislocations and Plastic Deformation in bcc Crystals


Describe the specialities of plastic deformation in bcc crystals. Consider glide systems, the role of screw dislocations    
Consider low temperature deformation; twinning as a deformation mode    
Applications, state of the art, outlook    
Defects in Quasicrystals (Nobel Prize 2011)
   
History, general background for periodic tilings in 2 Dimensions    
Quasicrystal as projections from 6-dim. crystals    
Point defects and diffusion, Phasons and quasi-dislocations, State of the art and problems