Magnetization reversal and stress effects in a FeCoSiB ME sensor film
Magnetization reversal in the ferromagnetic FeCoSiB layer for ME sensors
Complementary domain movies taken simultaneously with orthogonal aligned magneto-optical sensitivity directions.
T. von Hofe, N. O. Urs, B. Mozooni, T. Jansen, C. Kirchhof, D. E. Bürgler, E. Quandt, J. McCord, Dual wavelength magneto-optical imaging of magnetic thin films, Applied Physics Letters 103, 142410 (2013)