MOIF imaging on ferrites
Magneto-optical indicator film exposing the inner magnetic domain structure of a single-crystal CoFe2O4.
M. Abes, C. T. Koops, S. B. Hrkac, J. McCord, N. O. Urs, N. Wolff, L. Kienle, W. J. Ren, L. Bouchenoire, B. M. Murphy, O. M. Magnussen. Domain structure and reorientation in CoFe2O4, Phys. Rev. B 93, 195427 (2016)