2010
- H. Jacobsen, K. Prume, B. Wagner, K. Ortner, T. Jung
High-rate sputtering of thick PZT thin films for MEMS,
Journal of Electroceramics, 25 (2010) 198–202
- H. Greve, E. Woltermann, H.-J. Quenzer, B. Wagner, and E. Quandt
Giant magnetoelectric coefficients in (Fe90Co10)78Si12B10 - AlN thinfilm composites
Applied Physics Letters 96, 182501 (2010)
- H. Greve, E. Woltermann, R. Jahns, S. Marauska, B. Wagner, R. Knöchel, M. Wuttig and E. Quandt, Low damping resonant magnetoelectric sensors