Thin film recording head

Polar magnetization component observed at the air bearing surface of a thin film recording head with sub-µm pole-tip width in a simulated write process.

B. Argyle, J. McCord, Efficient Kerr microscopy, Magnetic Storage Systems Beyond 2000 - Nato Science Series: II: Mathematics, Physics and Chemistry, vol. 41 ed. G.C. Hadjipanayis (2001)