Magnetization dynamics - time resolved microscopy
Time resolved Kerr microscopy with psec time-resolution
Lateral and temporal evolution of the change of magnetization along and perpendicular to the fast pulse field direction.
U. Queitsch, J. McCord, A. Neudert, R. Schäfer, L. Schultz, K. Rott, H. Brückl, Domain wall induced modes of high-frequency response in ferromagnetic elements, J. Appl. Phys. 100, 093911 (2006)