Cross-tie domain wall structures in exchange bias systems
Variable cross-tie domain wall structures in exchange bias thin films
Cross-tie domain wall structures in a Ni81Fe19/NiO bilayer. Different domain wall structures are observed along the descending and ascending loop branches. The magneto-optical sensitivity is aligned vertically
J. McCord, R. Schäfer, Domain wall asymmetries in Ni81Fe19/NiO: proof of variable anisotropies in exchange bias systems, New Journal of Physics 11, 83016 (2009)