Functional Nanomaterials Chair

Publications

296 Zhang, RY; Wu, W.Z.; Bowen, C.; Basset, P.; Falconi, C.; Borras, A.; Konstantinidis, S.; Adelung, R.; Ventura, J.

"Triboelectric and piezoelectric advances in Europe and North America"

(2024) , 120, Art.No. 109113

NANO ENERGY

 

295 Schadte, P; Rademacher, F.; Andresen, G.; Hellfritzsch, M.; Qiu, H.Y.; Maschkowitz, G.; Gläser, R.; Heinemann, N.; Drücke, D.; Fickenscher, H.; Scherliess, R.; Harder, J.; Adelung, R.; Siebert, L.

"3D-printed wound dressing platform for protein administration based on alginate and zinc oxide tetrapods"

(2023) , 10 (1), Art.No. 53

NANO CONVERGENCE

 

294 Saure, LM; Kohlmann, N.; Qiu, H.Y.; Shetty, S.; Nia, A.S.; Ravishankar, N.; Feng, X.L.; Szameit, A.; Kienle, L.; Adelung, R.; Schütt, F.

"Hybrid Aeromaterials for Enhanced and Rapid Volumetric Photothermal Response"

(2023) , 17 (22), pp. 22444-22455

ACS NANO

 

293 Terasa, MI; Birkoben, T.; Noll, M.; Adejube, B.; Madurawala, R.; Carstens, N.; Strunskus, T.; Kaps, S.; Faupel, F.; Vahl, A.; Kohlstedt, H.; Adelung, R.

"Pathways towards truly brain-like computing primitives"

(2023) , 69, pp. 41-53

MATERIALS TODAY

 

292 Molaiyan, P; Abdollahifar, M.; Boz, B.; Beutl, A.; Krammer, M.; Zhang, N.X.; Tron, A.; Romio, M.; Ricci, M.; Adelung, R.; Kwade, A.; Lassi, U.; Paolella, A.

"Optimizing Current Collector Interfaces for Efficient "Anode-Free" Lithium Metal Batteries"

(2023)

ADVANCED FUNCTIONAL MATERIALS

 

291 Jungbluth, J; Bruns, S.; Schmidt, C.; Beckmann, F.; Moosmann, J.; Gapeeva, A.; Carstensen, J.; Adelung, R.; Zeller-Plumhoff, B.; Gurka, M.

"Interface failure analysis of embedded NiTi SMA wires using in situ high-resolution X-ray synchrotron tomography"

(2023) , 205, Art.No. 113345

MATERIALS CHARACTERIZATION

 

290 Harden, F; Schädel, B.; Siegel, M.; Kral, R.; Adelung, R.; Jacobs, O.

"Proof of Concept: In-Situ Wear Differentiation of Simultaneously Wearing Counterparts"

(2023) , 71 (3), Art.No. 89

TRIBOLOGY LETTERS

 

289 Hauck, M; Saure, L.M.; Zeller-Plumhoff, B.; Kaps, S.; Hammel, J.; Mohr, C.; Rieck, L.; Nia, A.S.; Feng, X.L.; Pugno, N.M.; Adelung, R.; Schütt, F.

"Overcoming Water Diffusion Limitations in Hydrogels via Microtubular Graphene Networks for Soft Actuators"

(2023) , 35 (41)

ADVANCED MATERIALS

 

288 Poschmann, MPM; Siebert, L.; Lupan, C.; Lupan, O.; Schütt, F.; Adelung, R.; Stock, N.

"Surface Conversion of ZnO Tetrapods Produces Pinhole-Free ZIF-8 Layers for Selective and Sensitive H2 Sensing Even in Pure Methane"

(2023) , 15 (32), pp. 38674-38681

ACS APPLIED MATERIALS & INTERFACES

 

287 Teegen, IS; Schadte, P.; Wille, S.; Adelung, R.; Siebert, L.; Kern, M.

"Comparison of properties and cost efficiency of zirconia processed by DIW printing, casting and CAD/CAM-milling"

(2023) , 39 (7), pp. 669-676

DENTAL MATERIALS

 

286 Kubelt, C; Hellmold, D.; Peschke, E.; Hauck, M.; Will, O.; Schütt, F.; Lucius, R.; Adelung, R.; Scherliess, R.; Hövener, J.B.; Jansen, O.; Synowitz, M.; Held-Feindt, J.

"Establishment of a Rodent Glioblastoma Partial Resection Model for Chemotherapy by Local Drug Carriers-Sharing Experience"

(2023) , 11 (6), Art.No. 1518

BIOMEDICINES

 

285 Liserre, M; Pascal, Y.; McCord, J.; Pereira, T.; Adelung, R.; Zimoch, L.; Kaps, S.; Li, X.X.; Sun, N.X.

"Voltage Controlled Magnetic Components for Power Electronics"

(2023) , 10 (2), pp. 40-48

IEEE POWER ELECTRONICS MAGAZINE

 

284 Lupan, O; Magariu, N.; Santos-Carballal, D.; Ababii, N.; Offermann, J.; Pooker, P.; Hansen, S.; Siebert, L.; de Leeuw, N.H.; Adelung, R.

"Development of 2-in-1 Sensors for the Safety Assessment of Lithium-Ion Batteries via Early Detection of Vapors Produced by Electrolyte Solvents"

(2023) , 15 (22), pp. 27340-27356

ACS APPLIED MATERIALS & INTERFACES

 

283 Harden, F; Kral, R.; Schädel, B.; Adelung, R.; Jacobs, O.

"Fabrication of precise non-assembly mechanisms by multi-material fused layer modeling and subsequent heat treatment"

(2023)

ENGINEERING REPORTS

 

282 Jin, I; Strobel, J.; Schümann, U.; Ciobanu, V.; Ursaki, V.; Gorceac, L.; Cinic, B.; Himcinschi, C.; Adelung, R.; Kienle, L.; Tiginyanu, I.

"Versatile self-catalyzed growth of freestanding zinc blende/wurtzite InP nanowires on an aerographite substrate for single-nanowire light detection"

(2023) , 48 (9), pp. 881-889

MRS BULLETIN

 

281 Hellmold, D; Kubelt, C.; Daunke, T.; Beckinger, S.; Janssen, O.; Hauck, M.; Schütt, F.; Adelung, R.; Lucius, R.; Haag, J.; Sebens, S.; Synowitz, M.; Held-Feindt, J.

"Sequential Treatment with Temozolomide Plus Naturally Derived AT101 as an Alternative Therapeutic Strategy: Insights into Chemoresistance Mechanisms of Surviving Glioblastoma Cells"

(2023) , 24 (10), Art.No. 9075

INTERNATIONAL JOURNAL OF MOLECULAR SCIENCES

 

280 Brinza, M; Schröeder, S.; Ababii, N.; Gronenberg, M.; Strunskus, T.; Pauporte, T.; Adelung, R.; Faupel, F.; Lupan, O.

"Two-in-One Sensor Based on PV4D4-Coated TiO2 Films for Food Spoilage Detection and as a Breath Marker for Several Diseases"

(2023) , 13 (5), Art.No. 538

BIOSENSORS-BASEL

 

279 Santos-Carballal, D; Lupan, O.; Magariu, N.; Ababii, N.; Krüger, H.; Bodduluri, M.T.; de Leeuw, N.H.; Hansen, S.; Adelung, R.

"Al2O3/ZnO composite-based sensors for battery safety applications: An experimental and theoretical investigation"

(2023) , 109, Art.No. 108301

NANO ENERGY

 

278 Barg, I; Kohlmann, N.; Rasch, F.; Strunskus, T.; Adelung, R.; Kienle, L.; Faupel, F.; Schroeder, S.; Schuett, F.

"Strain-Invariant, Highly Water Stable All-Organic Soft Conductors Based on Ultralight Multi-Layered Foam-Like Framework Structures"

(2023) , 33 (21)

ADVANCED FUNCTIONAL MATERIALS

 

277 Krüger, H; Cavers, H.; Offermann, J.; Polonskyi, O.; Adelung, R.; Hansen, S.

"Effects of Lithium Polysulfides on the Formation of Solid Electrolyte Interfaces in Silicon Anodes"

(2023)

ACS APPLIED MATERIALS & INTERFACES

 

276 Gapeeva, A; Qiu, H.Y.; Cojocaru, A.; Arndt, C.; Riaz, T.; Schütt, F.; Selhuber-Unkel, C.; Mishra, Y.K.; Tura, A.; Sonntag, S.; Gniesmer, S.; Grisanti, S.; Kaps, S.; Adelung, R.

"Tetrapodal ZnO-Based Composite Stents for Minimally Invasive Glaucoma Surgery"

(2023) , 9 (3), pp. 1352-1361

ACS BIOMATERIALS SCIENCE & ENGINEERING

 

275 Wolff, N; Braniste, T.; Krüger, H.; Mangelsen, S.; Islam, R.; Schürmann, U.; Saure, L.M.; Schütt, F.; Hansen, S.; Terraschke, H.; Adelung, R.; Tiginyanu, I.; Kienle, L.

"Synthesis and Nanostructure Investigation of Hybrid β-Ga2O3/ZnGa2O4 Nanocomposite Networks with Narrow-Band Green Luminescence and High Initial Electrochemical Capacity"

(2023) , 19 (18)

SMALL

 

274 Büter, A; Maschkowitz, G.; Baum, M.; Mishra, Y.K.; Siebert, L.; Adelung, R.; Fickenscher, H.

"Antibacterial Activity of Nanostructured Zinc Oxide Tetrapods"

(2023) , 24 (4), Art.No. 3444

INTERNATIONAL JOURNAL OF MOLECULAR SCIENCES

 

273 Schröder, S; Ababii, N.; Brînza, M.; Magariu, N.; Zimoch, L.; Bodduluri, M.T.; Strunskus, T.; Adelung, R.; Faupel, F.; Lupan, O.

"Tuning the Selectivity of Metal Oxide Gas Sensors with Vapor Phase Deposited Ultrathin Polymer Thin Films"

(2023) , 15 (3), Art.No. 524

POLYMERS

 

272 Gapeeva, A; Vogtmann, J.; Zeller-Plumhoff, B.; Beckmann, F.; Gurka, M.; Carstensen, J.; Adelung, R.

""Electrochemical Surface Structuring for Strong SMA Wire-Polymer Interface Adhesion" (vol 13, pg 21924, 2021)"

(2023) , 15 (3), pp. 4860-4861

ACS APPLIED MATERIALS & INTERFACES

 

271 Li, JF; Reimers, A.; Dang, K.M.; Brunk, M.G.K.; Drewes, J.; Hirsch, U.M.; Willems, C.; Schmelzer, C.E.H.; Groth, T.; Nia, A.S.; Feng, X.L.; Adelung, R.; Sacher, W.D.; Schütt, F.; Poon, J.K.S.

"3D printed neural tissues with in situ optical dopamine sensors"

(2023) , 222, Art.No. 114942

BIOSENSORS & BIOELECTRONICS

 

270 Zacharias, HU; Kaleta, C.; Cossais, F.; Schaeffer, E.; Berndt, H.; Best, L.; Dost, T.; Gluesing, S.; Groussin, M.; Poyet, M.; Heinzel, S.; Bang, C.; Siebert, L.; Demetrowitsch, T.; Leypoldt, F.; Adelung, R.; Bartsch, T.; Bosy-Westphal, A.; Schwarz, K.; Berg, D.

"Microbiome and Metabolome Insights into the Role of the Gastrointestinal-Brain Axis in Parkinson's and Alzheimer's Disease: Unveiling Potential Therapeutic Targets"

(2022) , 12 (12), Art.No. 1222

METABOLITES

 

269 Veys, E; Makower, L.; Williamson, M.; Saure, L.M.; Adelung, R.; Schütt, F.; Pugno, N.M.; Marrow, T.J.

"In situ observation of compressive deformation of an interconnected network of zinc oxide tetrapods"

(2023) , 224, Art.No. 115153

SCRIPTA MATERIALIA

 

268 Sonntag, SR; Gniesmer, S.; Gapeeva, A.; Offermann, K.J.; Adelung, R.; Mishra, Y.K.; Cojocaru, A.; Kaps, S.; Grisanti, S.; Grisanti, S.; Tura, A.

"In Vitro Evaluation of Zinc Oxide Tetrapods as a New Material Component for Glaucoma Implants"

(2022) , 12 (11), Art.No. 1805

LIFE-BASEL

 

267 Sonntag, SR; Gniesmer, S.; Gapeeva, A.; Adelung, R.; Cojocaru, A.; Mishra, Y.K.; Kaps, S.; Tura, A.; Grisanti, S.; Grisanti, S.; Nassar, K.

"Zinc Oxide Tetrapods Modulate Wound Healing and Cytokine Release In Vitro-A New Antiproliferative Substance in Glaucoma Filtering Surgery"

(2022) , 12 (11), Art.No. 1691

LIFE-BASEL

 

266 Marxen, ML; Hansen, L.; Reimers, A.; Tjardts, T.; Saure, L.M.; Greve, E.; Drewes, J.; Schütt, F.; Adelung, R.; Kersten, H.

"On the plasma permeability of highly porous ceramic framework materials using polymers as marker materials"

(2023) , 20 (1)

PLASMA PROCESSES AND POLYMERS

 

265 Lupan, C; Mishra, A.K.; Wolff, N.; Drewes, J.; Krüger, H.; Vahl, A.; Lupan, O.; Pauporté, T.; Viana, B.; Kienle, L.; Adelung, R.; de Leeuw, N.H.; Hansen, S.

"Nanosensors Based on a Single ZnO:Eu Nanowire for Hydrogen Gas Sensing"

(2022)

ACS APPLIED MATERIALS & INTERFACES

 

264 Lupan, O; Santos-Carballal, D.; Magariu, N.; Mishra, A.K.; Ababii, N.; Krüger, H.; Wolff, N.; Vahl, A.; Bodduluri, M.T.; Kohlmann, N.; Kienle, L.; Adelung, R.; de Leeuw, N.H.; Hansen, S.

"Al2O3/ZnO Heterostructure-Based Sensors for Volatile Organic Compounds in Safety Applications"

(2022) , 14 (25), pp. 29331-29344

ACS APPLIED MATERIALS & INTERFACES

 

263 Ohmes, J; Saure, L.M.; Schütt, F.; Trenkel, M.; Seekamp, A.; Scherliess, R.; Adelung, R.; Fuchs, S.

"Injectable Thermosensitive Chitosan-Collagen Hydrogel as A Delivery System for Marine Polysaccharide Fucoidan"

(2022) , 20 (6), Art.No. 402

MARINE DRUGS

 

262 Hauck, M; Hellmold, D.; Kubelt, C.; Synowitz, M.; Adelung, R.; Schütt, F.; Held-Feindt, J.

"Localized Drug Delivery Systems in High-Grade Glioma Therapy-From Construction to Application"

(2022) , 5 (8), Art.No. 2200013

ADVANCED THERAPEUTICS

 

261 Greijer, H; Mirotta, N.; Treossi, E.; Valorosi, F.; Schütt, F.; Siebert, L.; Mishra, Y.K.; Adelung, R.; Palermo, V.; Hillborg, H.

"Tuneable conductivity at extreme electric fields in ZnO tetrapod-silicone composites for high-voltage power cable insulation"

(2022) , 12 (1), Art.No. 6035

SCIENTIFIC REPORTS

 

260 Hauck, M; Dittmann, J.; Zeller-Plumhoff, B.; Madurawala, R.; Hellmold, D.; Kubelt, C.; Synowitz, M.; Held-Feindt, J.; Adelung, R.; Wulfinghoff, S.; Schütt, F.

"Fabrication and Modelling of a Reservoir-Based Drug Delivery System for Customizable Release"

(2022) , 14 (4), Art.No. 777

PHARMACEUTICS

 

259 Terasa, MI; Holtz, P.; Carstens, N.; Kaps, S.; Faupel, F.; Vahl, A.; Adelung, R.

"Sparse CNT networks with implanted AgAu nanoparticles: A novel memristor with short-term memory bordering between diffusive and bipolar switching"

(2022) , 17 (3), Art.No. e0264846

PLOS ONE

 

258 Wang, FL; Saure, L.M.; Schütt, F.; Lorich, F.; Rasch, F.; Nia, A.S.; Feng, X.L.; Seekamp, A.; Klüter, T.; Naujokat, H.; Adelung, R.; Fuchs, S.

"Graphene Oxide Framework Structures and Coatings: Impact on Cell Adhesion and Pre-Vascularization Processes for Bone Grafts"

(2022) , 23 (6), Art.No. 3379

INTERNATIONAL JOURNAL OF MOLECULAR SCIENCES

 

257 Qiu, HY; Feng, K.; Gapeeva, A.; Meurisch, K.; Kaps, S.; Li, X.; Yu, L.M.; Mishra, Y.K.; Adelung, R.; Baum, M.

"Functional polymer materials for modern marine biofouling control"

(2022) , 127, Art.No. 101516

PROGRESS IN POLYMER SCIENCE

 

256 Qiu, HY; Gapeeva, A.; Hölken, I.; Kaps, S.; Adelung, R.; Baum, M.J.

"Preventing algae adhesion using lubricant-modified polydimethylsiloxane/polythiourethane nanocomposite"

(2022) , 214, Art.No. 110389

MATERIALS & DESIGN

 

255 Kohlmann, N; Hansen, L.; Lupan, C.; Schürmann, U.; Reimers, A.; Schütt, F.; Adelung, R.; Kersten, H.; Kienle, L.

"Fabrication of ZnO Nanobrushes by H2-C2H2 Plasma Etching for H2 Sensing Applications"

(2021) , 13 (51), pp. 61758-61769

ACS APPLIED MATERIALS & INTERFACES

 

254 Qiu, HY; Gapeeva, A.; Kaps, S.; Adelung, R.; Baum, M.J.

"Modification of Nylon Nets with Poly(dimethylsiloxane)/Tetrapodal-Shaped ZnO Composite for Aquaculture Biofouling Control"

(2021) , 3 (12), pp. 6598-6607

ACS APPLIED POLYMER MATERIALS

 

253 Schröder, S; Ababii, N.; Lupan, O.; Drewes, J.; Magariu, N.; Krüger, H.; Strunskus, T.; Adelung, R.; Hansen, S.; Faupel, F.

"Sensing performance of CuO/Cu2O/ZnO:Fe heterostructure coated with thermally stable ultrathin hydrophobic PV3D3 polymer layer for battery application"

(2022) , 23, Art.No. 100642

MATERIALS TODAY CHEMISTRY

 

252 Spratte, T; Arndt, C.; Wacker, I.; Hauck, M.; Adelung, R.; Schröder, R.R.; Schütt, F.; Selhuber-Unkel, C.

"Thermoresponsive Hydrogels with Improved Actuation Function by Interconnected Microchannels"

(2022) , 4 (3), Art.No. 2100081

ADVANCED INTELLIGENT SYSTEMS

 

251 Schütt, F; Rasch, F.; Deka, N.; Reimers, A.; Saure, L.M.; Kaps, S.; Rank, J.; Carstensen, J.; Mishra, Y.K.; Misseroni, D.; Vázquez, A.R.; Lohe, M.R.; Nia, A.S.; Pugno, N.M.; Feng, X.L.; Adelung, R.

"Electrically powered repeatable air explosions using microtubular graphene assemblies"

(2021) , 48, pp. 7-17

MATERIALS TODAY

 

250 Siemsen, K; Rajput, S.; Rasch, F.; Taheri, F.; Adelung, R.; Lammerding, J.; Selhuber-Unkel, C.

"Tunable 3D Hydrogel Microchannel Networks to Study Confined Mammalian Cell Migration"

(2021) , 10 (23), Art.No. 2100625

ADVANCED HEALTHCARE MATERIALS

 

249 Hindenlang, B; Gapeeva, A.; Baum, M.J.; Kaps, S.; Saure, L.M.; Rasch, F.; Hammel, J.; Moosmann, J.; Storm, M.; Adelung, R.; Schütt, F.; Zeller-Plumhoff, B.

"Evaporation kinetics in highly porous tetrapodal zinc oxide networks studied using in situ SRμCT"

(2021) , 11 (1), Art.No. 20272

SCIENTIFIC REPORTS

 

248 Nasajpour, A; Samandari, M.; Patil, C.D.; Abolhassani, R.; Suryawanshi, R.K.; Adelung, R.; Rubahn, H.G.; Khademhosseini, A.; Mishra, Y.K.; Shukla, D.; Tamayol, A.; Weiss, P.S.

"Nanoengineered Antiviral Fibrous Arrays with Rose-Thorn-Inspired Architectures"

(2021) , 3 (11), pp. 1566-1571

ACS MATERIALS LETTERS

 

247 Qiu, HY; Schmidt, C.; Carstensen, J.; Kaps, S.; Adelung, R.

"Nanoscale-Sculptured Al Microparticles as Universal Hierarchical Adhesion Promoters"

(2021) , 15 (10), Art.No. 2100296

PHYSICA STATUS SOLIDI-RAPID RESEARCH LETTERS

 

246 Braniste, T; Ciobanu, V.; Schütt, F.; Mimura, H.; Raevschi, S.; Adelung, R.; Pugno, N.M.; Tiginyanu, I.

"Self-Propelled Aero-GaN Based Liquid Marbles Exhibiting Pulsed Rotation on the Water Surface"

(2021) , 14 (17), Art.No. 5086

MATERIALS

 

245 Lupan, O; Krüger, H.; Siebert, L.; Ababii, N.; Kohlmann, N.; Buzdugan, A.; Bodduluri, M.T.; Magariu, N.; Terasa, M.I.; Strunskus, T.; Kienle, L.; Adelung, R.; Hansen, S.

"Additive Manufacturing as a Means of Gas Sensor Development for Battery Health Monitoring"

(2021) , 9 (9), Art.No. 252

CHEMOSENSORS

 

244 Jordt, P; Wolff, N.; Hrkac, S.B.; Shree, S.; Wang, D.; Harder, R.J.; Kübel, C.; Adelung, R.; Shpyrko, O.G.; Magnussen, O.M.; Kienle, L.; Murphy, B.M.

"Visualizing Intrinsic 3D-Strain Distribution in Gold Coated ZnO Microstructures by Bragg Coherent X-Ray Diffraction Imaging and Transmission Electron Microscopy with Respect to Piezotronic Applications"

(2021) , 7 (11), Art.No. 2100546

ADVANCED ELECTRONIC MATERIALS

 

243 Singh, U; Saifi, Z.; Kumar, M.; Reimers, A.; Krishnananda, S.D.; Adelung, R.; Baum, M.

"Role of structural specificity of ZnO particles in preserving functionality of proteins in their corona"

(2021) , 11 (1), Art.No. 15945

SCIENTIFIC REPORTS

 

242 Lupan, O; Santos-Carballal, D.; Ababii, N.; Magariu, N.; Hansen, S.; Vahl, A.; Zimoch, L.; Hoppe, M.; Pauporté, T.; Galstyan, V.; Sontea, V.; Chow, L.; Faupel, F.; Adelung, R.; de Leeuw, N.H.; Comini, E.

"TiO2/Cu2O/CuO Multi-Nanolayers as Sensors for H2 and Volatile Organic Compounds: An Experimental and Theoretical Investigation"

(2021) , 13 (27), pp. 32363-32380

ACS APPLIED MATERIALS & INTERFACES

 

241 Qiu, HY; Gapeeva, A.; Kaps, S.; Adelung, R.; Baum, M.

"Core-shell structured nets for biofouling control in aquaculture"

(2021) , 21, Art.No. 100781

AQUACULTURE REPORTS

 

240 Siebert, S; Meurisch, K.; Bernholt, S.; Adelung, R.; Parchmann, I.

"From water strider to research - interrelationships of structure and characteristics from three perspectives"

(2023) , 30 (1), pp. 13-22

CHEMKON

 

239 Hansen, S; Hahn, F.; Krueger, H.; Andresen, M.; Adelung, R.; Liserre, M.

"Reliability of Silicon Battery Technology and Power Electronics Based Energy Conversion"

(2021) , 8 (2), pp. 60-69

IEEE POWER ELECTRONICS MAGAZINE

 

238 Lupan, O; Ababii, N.; Mishra, A.K.; Bodduluri, M.T.; Magariu, N.; Vahl, A.; Krüger, H.; Wagner, B.; Faupel, F.; Adelung, R.; de Leeuw, N.H.; Hansen, S.

"Heterostructure-based devices with enhanced humidity stability for H2 gas sensing applications in breath tests and portable batteries"

(2021) , 329, Art.No. 112804

SENSORS AND ACTUATORS A-PHYSICAL

 

237 Jordt, P; Hrkac, S.B.; Gröttrup, J.; Davydok, A.; Krywka, C.; Wolff, N.; Kienle, L.; Adelung, R.; Magnussen, O.M.; Murphy, B.M.

"Local Strain Distribution in ZnO Microstructures Visualized with Scanning Nano X-Ray Diffraction and Impact on Electrical Properties"

(2021) , 23 (11), Art.No. 2100201

ADVANCED ENGINEERING MATERIALS

 

236 Gapeeva, A; Vogtmann, J.; Zeller-Plumhoff, B.; Beckmann, F.; Gurka, M.; Carstensen, J.; Adelung, R.

"Electrochemical Surface Structuring for Strong SMA Wire-Polymer Interface Adhesion"

(2021) , 13 (18), pp. 21924-21935

ACS APPLIED MATERIALS & INTERFACES

 

235 Rodrigues, J; Becker, C.; Ben Sedrine, N.; Kamp, M.; Kienle, L.; Adelung, R.; Mishra, Y.K.; Parak, W.J.; Chakraborty, I.; Correia, M.R.; Monteiro, T.

"Luminescent silver nanoclusters decorated on ZnO tetrapods: a detailed understanding of their role in photoluminescence features"

(2021) , 9 (22)

JOURNAL OF MATERIALS CHEMISTRY C

 

234 Plesco, I; Ciobanu, V.; Braniste, T.; Ursaki, V.; Rasch, F.; Sarua, A.; Raevschi, S.; Adelung, R.; Dutta, J.; Tiginyanu, I.

"Highly Porous and Ultra-Lightweight Aero-Ga2O3: Enhancement of Photocatalytic Activity by Noble Metals"

(2021) , 14 (8), Art.No. 1985

MATERIALS

 

233 Postica, V; Lupan, O.; Gapeeva, A.; Hansen, L.; Khaledialidusti, R.; Mishra, A.K.; Drewes, J.; Kersten, H.; Faupel, F.; Adelung, R.; Hansen, S.

"Improved Long-Term Stability and Reduced Humidity Effect in Gas Sensing: SiO2 Ultra-Thin Layered ZnO Columnar Films"

(2021) , 6 (5), Art.No. 2001137

ADVANCED MATERIALS TECHNOLOGIES

 

232 Arndt, C; Hauck, M.; Wacker, I.; Zeller-Plumhoff, B.; Rasch, F.; Taale, M.; Nia, A.S.; Feng, X.L.; Adelung, R.; Schröder, R.R.; Schütt, F.; Selhuber-Unkel, C.

"Microengineered Hollow Graphene Tube Systems Generate Conductive Hydrogels with Extremely Low Filler Concentration"

(2021) , 21 (8), pp. 3690-3697

NANO LETTERS

 

231 Siebert, L; Luna-Cerón, E.; García-Rivera, L.E.; Oh, J.; Jang, J.; Rosas-Gómez, D.A.; Pérez-Gómez, M.D.; Maschkowitz, G.; Fickenscher, H.; Oceguera-Cuevas, D.; Holguín-León, C.G.; Byambaa, B.; Hussain, M.A.; Enciso-Martínez, E.; Cho, M.; Lee, Y.; Sobahi, N.; Hasan, A.; Orgill, D.P.; Mishra, Y.K.; Adelung, R.; Lee, E.; Shin, S.R.

"Light-Controlled Growth Factors Release on Tetrapodal ZnO-Incorporated 3D-Printed Hydrogels for Developing Smart Wound Scaffold"

(2021) , 31 (22), Art.No. 2007555

ADVANCED FUNCTIONAL MATERIALS

 

230 Lupan, O; Magariu, N.; Khaledialidusti, R.; Mishra, A.K.; Hansen, S.; Krüger, H.; Postica, V.; Heinrich, H.; Viana, B.; Ono, L.K.; Cuenya, B.R.; Chow, L.; Adelung, R.; Pauporté, T.

"Comparison of Thermal Annealing versus Hydrothermal Treatment Effects on the Detection Performances of ZnO Nanowires"

(2021) , 13 (8), pp. 10537-10552

ACS APPLIED MATERIALS & INTERFACES

 

229 Klemm, S; Baum, M.; Qiu, H.Y.; Nan, Z.B.; Cavalheiro, M.; Teixeira, M.C.; Tendero, C.; Gapeeva, A.; Adelung, R.; Dague, E.; Castelain, M.; Formosa-Dague, C.

"Development of Polythiourethane/ZnO-Based Anti-Fouling Materials and Evaluation of the Adhesion of Staphylococcus aureus and Candida glabrata Using Single-Cell Force Spectroscopy"

(2021) , 11 (2), Art.No. 271

NANOMATERIALS

 

228 Qiu, HY; Gapeeva, A.; Hölken, I.; Kaps, S.; Adelung, R.; Baum, M.J.

"Polydimethylsiloxane Microdomains Formation at the Polythiourethane/Air Interface and Its Influence on Barnacle Release"

(2021) , 13 (3), pp. 4545-4552

ACS APPLIED MATERIALS & INTERFACES

 

227 Rezvani, SJ; D'Elia, A.; Macis, S.; Nannarone, S.; Lupi, S.; Schütt, F.; Rasch, F.; Adelung, R.; Lu, B.; Zhang, Z.; Qu, L.; Feng, X.; Vázquez, A.R.; Marcelli, A.

"Structural anisotropy in three dimensional macroporous graphene: A polarized XANES investigation"

(2021) , 111, Art.No. 108171

DIAMOND AND RELATED MATERIALS

 

226 Schmitt, C; Rasch, F.; Cossais, F.; Held-Feindt, J.; Lucius, R.; Vázquez, A.R.; Nia, A.S.; Lohe, M.R.; Feng, X.L.; Mishra, Y.K.; Adelung, R.; Schütt, F.; Hattermann, K.

"Glial cell responses on tetrapod-shaped graphene oxide and reduced graphene oxide 3D scaffolds in brain in vitro and ex vivo models of indirect contact"

(2021) , 16 (1), Art.No. 015008

BIOMEDICAL MATERIALS

 

225 Kalu, CO; Hoppe, M.; Hölken, I.; Baytekin-Gerngross, M.; Gerngross, M.D.; Carstensen, J.; Adelung, R.

"Formation of micro-mechanical interlocking sites by nanoscale sculpturing for composites or hybrid materials with stainless steel"

(2020) , 35 (23-24), Art.No. PII S0884291420002848-3156

JOURNAL OF MATERIALS RESEARCH

 

224 Zhang, H; Horvat, J.; Lewis, R.A.; Adelung, R.; Fiedler, B.; Mishra, Y.K.

"Aerographite phonon density of states affects double resonant Raman scattering"

(2020) , 128 (19), Art.No. 195101

JOURNAL OF APPLIED PHYSICS

 

223 Cavers, H; Krüger, H.; Polonskyi, O.; Schütt, F.; Adelung, R.; Hansen, S.

"Temperature-Dependent Vapor Infiltration of Sulfur into Highly Porous Hierarchical Three-Dimensional Conductive Carbon Networks for Lithium Ion Battery Applications"

(2020) , 5 (43), pp. 28196-28203

ACS OMEGA

 

222 Rasch, F; Postica, V.; Schütt, F.; Mishra, Y.K.; Nia, A.S.; Lohe, M.R.; Feng, X.L.; Adelung, R.; Lupan, O.

"Highly selective and ultra-low power consumption metal oxide based hydrogen gas sensor employing graphene oxide as molecular sieve"

(2020) , 320, Art.No. 128363

SENSORS AND ACTUATORS B-CHEMICAL

 

221 Lupan, O; Ababii, N.; Mishra, A.K.; Gronenberg, O.; Vahl, A.; Schürmann, U.; Duppel, V.; Krüger, H.; Chow, L.; Kienle, L.; Faupel, F.; Adelung, R.; de Leeuw, N.H.; Hansen, S.

"Single CuO/Cu2O/Cu Microwire Covered by a Nanowire Network as a Gas Sensor for the Detection of Battery Hazards"

(2020) , 12 (37), pp. 42248-42263

ACS APPLIED MATERIALS & INTERFACES

 

220 Sharma, M; Poddar, M.; Gupta, Y.; Nigam, S.; Avasthi, D.K.; Adelung, R.; Abolhassani, R.; Fiutowski, J.; Joshi, M.; Mishra, Y.K.

"Solar light assisted degradation of dyes and adsorption of heavy metal ions from water by CuO-ZnO tetrapodal hybrid nanocomposite"

(2020) , 17, Art.No. 100336

MATERIALS TODAY CHEMISTRY

 

219 Vahl, A; Lupan, O.; Santos-Carballal, D.; Postica, V.; Hansen, S.; Cavers, H.; Wolff, N.; Terasa, M.I.; Hoppe, M.; Cadi-Essadek, A.; Dankwort, T.; Kienle, L.; de Leeuw, N.H.; Adelung, R.; Faupel, F.

"Surface functionalization of ZnO:Ag columnar thin films with AgAu and AgPt bimetallic alloy nanoparticles as an efficient pathway for highly sensitive gas discrimination and early hazard detection in batteries"

(2020) , 8 (32), pp. 16246-16264

JOURNAL OF MATERIALS CHEMISTRY A

 

218 Lupan, C; Khaledialidusti, R.; Mishra, A.K.; Postica, V.; Terasa, M.I.; Magariu, N.; Pauporté, T.; Viana, B.; Drewes, J.; Vahl, A.; Faupel, F.; Adelung, R.

"Pd-Functionalized ZnO:Eu Columnar Films for Room-Temperature Hydrogen Gas Sensing: A Combined Experimental and Computational Approach"

(2020) , 12 (22), pp. 24951-24964

ACS APPLIED MATERIALS & INTERFACES

 

217 Braniste, T; Dragoman, M.; Zhukov, S.; Aldrigo, M.; Ciobanu, V.; Iordanescu, S.; Alyabyeva, L.; Fumagalli, F.; Ceccone, G.; Raevschi, S.; Schütt, F.; Adelung, R.; Colpo, P.; Gorshunov, B.; Tiginyanu, I.

"Aero-Ga2O3Nanomaterial Electromagnetically Transparent from Microwaves to Terahertz for Internet of Things Applications"

(2020) , 10 (6), Art.No. 1047

NANOMATERIALS

 

216 Plesco, I; Braniste, T.; Wolff, N.; Gorceac, L.; Duppel, V.; Cinic, B.; Mishra, Y.K.; Sarua, A.; Adelung, R.; Kienle, L.; Tiginyanu, I.

"Aero-ZnS architectures with dual hydrophilic-hydrophobic properties for microfluidic applications"

(2020) , 8 (6), Art.No. 061105

APL MATERIALS

 

215 Rasch, F; Schmitt, C.; Saure, L.M.; Meyer, R.; Adamski, V.; Dengiz, D.; Scherliess, R.; Lucius, R.; Synowitz, M.; Mishra, Y.K.; Hattermann, K.; Adelung, R.; Held-Feindt, J.; Schütt, F.

"Macroscopic Silicone Microchannel Matrix for Tailored Drug Release and Localized Glioblastoma Therapy"

(2020) , 6 (6), pp. 3388-3397

ACS BIOMATERIALS SCIENCE & ENGINEERING

 

214 Colaco, R; Shree, S.; Siebert, L.; Appiah, C.; Dowds, M.; Schultzke, S.; Adelung, R.; Staubitz, A.

"Mechanochromic Microfibers Stabilized by Polymer Blending"

(2020) , 2 (5), pp. 2055-2062

ACS APPLIED POLYMER MATERIALS

 

213 Rodrigues, J; Hoppe, M.; Ben Sedrine, N.; Wolff, N.; Duppel, V.; Kienle, L.; Adelung, R.; Mishra, Y.K.; Correia, M.R.; Monteiro, T.

"ZnAl2O4 decorated Al-doped ZnO tetrapodal 3D networks: microstructure, Raman and detailed temperature dependent photoluminescence analysis"

(2020) , 2 (5), pp. 2114-2126

NANOSCALE ADVANCES

 

212 Siebert, L; Wolff, N.; Ababii, N.; Terasa, M.I.; Lupan, O.; Vahl, A.; Duppel, V.; Qiu, H.Y.; Tienken, M.; Mirabelli, M.; Sontea, V.; Faupel, F.; Kienle, L.; Adelung, R.

"Facile fabrication of semiconducting oxide nanostructures by direct ink writing of readily available metal microparticles and their application as low power acetone gas sensors"

(2020) , 70, Art.No. 104420

NANO ENERGY

 

211 Schütt, F; Zapf, M.; Signetti, S.; Strobel, J.; Krüger, H.; Röder, R.; Carstensen, J.; Wolff, N.; Marx, J.; Carey, T.; Schweichel, M.; Terasa, M.I.; Siebert, L.; Hong, H.K.; Kaps, S.; Fiedler, B.; Mishra, Y.K.; Lee, Z.; Pugno, N.M.; Kienle, L.; Ferrari, A.C.; Torrisi, F.; Ronning, C.; Adelung, R.

"Conversionless efficient and broadband laser light diffusers for high brightness illumination applications"

(2020) , 11 (1), Art.No. 1437

NATURE COMMUNICATIONS

 

210 Schmitt, C; Adamski, V.; Rasch, F.; Adelung, R.; Lucius, R.; Synowitz, M.; Hattermann, K.; Held-Feindt, J.

"Establishment of a glioblastoma in vitro (in)complete resection dual co-culture model suitable for drug testing"

(2020) , 228, Art.No. 151440

ANNALS OF ANATOMY-ANATOMISCHER ANZEIGER

 

209 De Nicola, F; Viola, I.; Tenuzzo, L.D.; Rasch, F.; Lohe, M.R.; Nia, A.S.; Schütt, F.; Feng, X.L.; Adelung, R.; Lupi, S.

"Wetting Properties of Graphene Aerogels"

(2020) , 10 (1), Art.No. 1916

SCIENTIFIC REPORTS

 

208 Shree, S; Dowds, M.; Kuntze, A.; Mishra, Y.K.; Staubitz, A.; Adelung, R.

"Self-reporting mechanochromic coating: a glassfiber reinforced polymer composite that predicts impact induced damage"

(2020) , 7 (2), pp. 598-604

MATERIALS HORIZONS

 

207 Tao, X; Jin, H.; Mintken, M.; Wolff, N.; Wang, Y.; Tao, R.; Li, Y.F.; Torun, H.; Xie, J.; Luo, J.T.; Zhou, J.; Wu, Q.; Dong, S.R.; Luo, J.K.; Kienle, L.; Adelung, R.; Mishra, Y.K.; Fu, Y.Q.

"Three-Dimensional Tetrapodal ZnO Microstructured Network Based Flexible Surface Acoustic Wave Device for Ultraviolet and Respiration Monitoring Applications"

(2020) , 3 (2), pp. 1468-1478

ACS APPLIED NANO MATERIALS

 

206 Yuksel, R; Buyukcakir, O.; Panda, P.K.; Lee, S.H.; Jiang, Y.; Singh, D.; Hansen, S.; Adelung, R.; Mishra, Y.K.; Ahuja, R.; Ruoff, R.S.

"Necklace-like Nitrogen-Doped Tubular Carbon 3D Frameworks for Electrochemical Energy Storage"

(2020) , 30 (10), Art.No. 1909725

ADVANCED FUNCTIONAL MATERIALS

 

205 Wagner, JM; Carstensen, J.; Adelung, R.

"Fundamental Aspects Concerning the Validity of the Standard Equivalent Circuit for Large-Area Silicon Solar Cells"

(2020) , 217 (2), Art.No. 1900612

PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE

 

204 Wolff, N; Ciobanu, V.; Enachi, M.; Kamp, M.; Braniste, T.; Duppel, V.; Shree, S.; Raevschi, S.; Medina-Sánchez, M.; Adelung, R.; Schmidt, O.G.; Kienle, L.; Tiginyanu, I.

"Advanced Hybrid GaN/ZnO Nanoarchitectured Microtubes for Fluorescent Micromotors Driven by UV Light"

(2020) , 16 (2), Art.No. 1905141

SMALL

 

203 Braniste, T; Zhukov, S.; Dragoman, M.; Alyabyeva, L.; Ciobanu, V.; Aldrigo, M.; Dragoman, D.; Iordanescu, S.; Shree, S.; Raevschi, S.; Adelung, R.; Gorshunov, B.; Tiginyanu, I.

"Terahertz shielding properties of aero-GaN"

(2019) , 34 (12), Art.No. 12LT02

SEMICONDUCTOR SCIENCE AND TECHNOLOGY

 

202 Sharma, M; Joshi, M.; Nigam, S.; Avasthi, D.K.; Adelung, R.; Srivastava, S.K.; Mishra, Y.K.

"Efficient oil removal from wastewater based on polymer coated superhydrophobic tetrapodal magnetic nanocomposite adsorbent"

(2019) , 17, pp. 130-141

APPLIED MATERIALS TODAY

 

201 Rasch, F; Schütt, F.; Saure, L.M.; Kaps, S.; Strobel, J.; Polonskyi, O.; Nia, A.S.; Lohe, M.R.; Mishra, Y.K.; Faupel, F.; Kienle, L.; Feng, X.L.; Adelung, R.

"Wet-Chemical Assembly of 2D Nanomaterials into Lightweight, Microtube-Shaped, and Macroscopic 3D Networks"

(2019) , 11 (47), pp. 44652-44663

ACS APPLIED MATERIALS & INTERFACES

 

200 Lupan, O; Postica, V.; Pauporté, T.; Viana, B.; Terasa, M.I.; Adelung, R.

"Room temperature gas nanosensors based on individual and multiple networked Au-modified ZnO nanowires"

(2019) , 299, Art.No. 126977

SENSORS AND ACTUATORS B-CHEMICAL

 

199 Wolff, N; Hrkac, V.; Ditto, J.J.; Duppel, V.; Mishra, Y.K.; Johnson, D.C.; Adelung, R.; Kienle, L.

"Crystallography at the nanoscale: planar defects in ZnO nanospikes"

(2019) , 52, pp. 1009-1015

JOURNAL OF APPLIED CRYSTALLOGRAPHY

 

198 Lupan, O; Postica, V.; Wolff, N.; Su, J.; Labat, F.; Ciofini, I.; Cavers, H.; Adelung, R.; Polonskyi, O.; Faupel, F.; Kienle, L.; Viana, B.; Pauporté, T.

"Low-Temperature Solution Synthesis of Au-Modified ZnO Nanowires for Highly Efficient Hydrogen Nanosensors"

(2019) , 11 (35), pp. 32115-32126

ACS APPLIED MATERIALS & INTERFACES

 

197 Ghimpu, L; Lupan, O.; Postica, V.; Strobel, J.; Kienle, L.; Terasa, M.I.; Mintken, M.; Tiginyan, I.; Marx, J.; Fiedler, B.; Adelung, R.

"Individual CdS-covered aerographite microtubes for room temperature VOC sensing with high selectivity"

(2019) , 100, pp. 275-282

MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING

 

196 Lupan, O; Postica, V.; Pauporté, T.; Hoppe, M.; Adelung, R.

"UV nanophotodetectors: A case study of individual Au-modified ZnO nanowires"

(2019) , 296, pp. 400-408

SENSORS AND ACTUATORS A-PHYSICAL

 

195 Taale, M; Krüger, D.; Ossei-Wusu, E.; Schütt, F.; Rehman, M.A.U.; Mishra, Y.K.; Marx, J.; Stock, N.; Fiedler, B.; Boccaccini, A.R.; Willumeit-Römer, R.; Adelung, R.; Selhuber-Unkel, C.

"Systematically Designed Periodic Electrophoretic Deposition for Decorating 3D Carbon-Based Scaffolds with Bioactive Nanoparticles"

(2019) , 5 (9), pp. 4393-4404

ACS BIOMATERIALS SCIENCE & ENGINEERING

 

194 Postica, V; Vahl, A.; Santos-Carballal, D.; Dankwort, T.; Kienle, L.; Hoppe, M.; Cadi-Essadek, A.; de Leeuw, N.H.; Terasa, M.I.; Adelung, R.; Faupel, F.; Lupan, O.

"Tuning ZnO Sensors Reactivity toward Volatile Organic Compounds via Ag Doping and Nanoparticle Functionalization"

(2019) , 11 (34), pp. 31452-31466

ACS APPLIED MATERIALS & INTERFACES

 

193 Dragoman, M; Braniste, T.; Iordanescu, S.; Aldrigo, M.; Raevschi, S.; Shree, S.; Adelung, R.; Tiginyanu, I.

"Electromagnetic interference shielding in X-band with aero-GaN"

(2019) , 30 (34), Art.No. 34LT01

NANOTECHNOLOGY

 

192 Postica, V; Paulowicz, I.; Lupan, O.; Schütt, F.; Wolff, N.; Cojocaru, A.; Mishra, Y.K.; Kienle, L.; Adelung, R.

"The effect of morphology and functionalization on UV detection properties of ZnO networked tetrapods and single nanowires"

(2019) , 166, pp. 393-398

VACUUM

 

191 Siebert, L; Lupan, O.; Mirabelli, M.; Ababii, N.; Terasa, M.I.; Kaps, S.; Cretu, V.; Vahl, A.; Faupel, F.; Adelung, R.

"3D-Printed Chemiresistive Sensor Array on Nanowire CuO/Cu2O/Cu Heterojunction Nets"

(2019) , 11 (28), pp. 25508-25515

ACS APPLIED MATERIALS & INTERFACES

 

190 Wolff, N; Jordt, P.; Braniste, T.; Popa, V.; Monaico, E.; Ursaki, V.; Petraru, A.; Adelung, R.; Murphy, B.M.; Kienle, L.; Tiginyanu, I.

"Modulation of Electrical Conductivity and Lattice Distortions in Bulk HVPE-Grown GaN"

(2019) , 8 (8), pp. Q141-Q146

ECS JOURNAL OF SOLID STATE SCIENCE AND TECHNOLOGY

 

189 Ababii, N; Hoppe, M.; Shree, S.; Vahl, A.; Ulfa, M.; Pauporté, T.; Viana, B.; Cretu, V.; Magariu, N.; Postica, V.; Sontea, V.; Terasa, M.I.; Polonskyi, O.; Faupel, F.; Adelung, R.; Lupan, O.

"Effect of noble metal functionalization and film thickness on sensing properties of sprayed TiO2 ultra-thin films"

(2019) , 293, pp. 242-258

SENSORS AND ACTUATORS A-PHYSICAL

 

188 Schmitt, C; Rasch, F.; Lechanteur, A.; Siemsen, K.; Lucius, R.; Selhuber-Unkel, C.; Held-Feindt, J.; Piel, G.; Adelung, R.; Hattermann, K.

"Brain specific foreign body reactions of neuro implant materials in different in vitro models"

(2019) , 67, pp. E585-E585

GLIA

 

187 Siebert, L; Schaller, T.; Schütt, F.; Kaps, S.; Carstensen, J.; Shree, S.; Bahr, J.; Mishra, Y.K.; Sievers, H.H.; Adelung, R.

"Perfect polymer interlocking by spherical particles: capillary force shapes hierarchical composite undercuts"

(2019) , 4 (4), pp. 947-952

NANOSCALE HORIZONS

 

186 Pérez-Díaz, O; Quiroga-González, E.; Hansen, S.; Silva-González, N.R.; Carstensenb, J.; Adelung, R.

"Fabrication of silicon microwires by a combination of chemical etching steps and their analysis as anode material in Li-ion batteries"

(2019) , 34 (13), pp. 785-791

MATERIALS TECHNOLOGY

 

185 Vahl, A; Dittmann, J.; Jetter, J.; Veziroglu, S.; Shree, S.; Ababii, N.; Lupan, O.; Aktas, O.C.; Strunskus, T.; Quandt, E.; Adelung, R.; Sharma, S.K.; Faupel, F.

"The impact of O2/Ar ratio on morphology and functional properties in reactive sputtering of metal oxide thin films"

(2019) , 30 (23), Art.No. 235603

NANOTECHNOLOGY

 

184 Dragoman, M; Ciobanu, V.; Shree, S.; Dragoman, D.; Braniste, T.; Raevschi, S.; Dinescu, A.; Sarua, A.; Mishra, Y.K.; Pugno, N.; Adelung, R.; Tiginyanu, I.

"Sensing up to 40 atm Using Pressure-Sensitive Aero-GaN"

(2019) , 13 (6), Art.No. UNSP 1900012

PHYSICA STATUS SOLIDI-RAPID RESEARCH LETTERS

 

183 Marx, J; Berns, J.C.; Spille, C.; Mintken, M.; Adelung, R.; Schlüter, M.; Fiedler, B.

"Theoretical Computational Fluid Dynamics Study of the Chemical Vapor Deposition Process for the Manufacturing of a Highly Porous 3D Carbon Foam"

(2019) , 42 (6), pp. 1240-1246

CHEMICAL ENGINEERING & TECHNOLOGY

 

182 Gutekunst, SB; Siemsen, K.; Huth, S.; Möhring, A.; Hesseler, B.; Timmermann, M.; Paulowicz, I.; Mishra, Y.K.; Siebert, L.; Adelung, R.; Selhuber-Unkel, C.

"3D Hydrogels Containing Interconnected Microchannels of Subcellular Size for Capturing Human Pathogenic Acanthamoeba Castellanii"

(2019) , 5 (4), pp. 1784-1792

ACS BIOMATERIALS SCIENCE & ENGINEERING

 

181 Pöhls, JH; Schütt, F.; O'Neill, C.; Shree, S.; Johnson, M.B.; Mishra, Y.K.; Adelung, R.; White, M.A.

"Thermal and electrical transport properties in multi-walled carbon nanotube-coated ZnO tetrapods and self-entangled multi-walled carbon nanotube tubes"

(2019) , 144, pp. 423-432

CARBON

 

180 Rodrigues, J; Smazna, D.; Ben Sedrine, N.; Nogales, E.; Adelung, R.; Mishra, Y.K.; Mendez, B.; Correia, M.R.; Monteiro, T.

"Probing surface states in C60 decorated ZnO microwires: detailed photoluminescence and cathodoluminescence investigations"

(2019) , 1 (4), pp. 1516-1526

NANOSCALE ADVANCES

 

179 Smazna, D; Shree, S.; Polonskyi, O.; Lamaka, S.; Baum, M.; Zheludkevich, M.; Faupel, F.; Adelung, R.; Mishra, Y.K.

"Mutual interplay of ZnO micro- and nanowires and methylene blue during cyclic photocatalysis process"

(2019) , 7 (2), Art.No. 103016

JOURNAL OF ENVIRONMENTAL CHEMICAL ENGINEERING

 

178 Agelidis, A; Koujah, L.; Suryawanshi, R.; Yadavalli, T.; Mishra, Y.K.; Adelung, R.; Shukla, D.

"An Intra-Vaginal Zinc Oxide Tetrapod Nanoparticles (ZOTEN) and Genital Herpesvirus Cocktail Can Provide a Novel Platform for Live Virus Vaccine"

(2019) , 10, Art.No. 500

FRONTIERS IN IMMUNOLOGY

 

177 Marx, J; Lewke, M.R.D.; Smazna, D.; Mishra, Y.K.; Adelung, R.; Schulte, K.; Fiedler, B.

"Processing, growth mechanism and thermodynamic calculations of carbon foam with a hollow tetrapodal morphology - Aerographite"

(2019) , 470, pp. 535-542

APPLIED SURFACE SCIENCE

 

176 Vahl, A; Carstensen, J.; Kaps, S.; Lupan, O.; Strunskus, T.; Adelung, R.; Faupel, F.

"Concept and modelling of memsensors as two terminal devices with enhanced capabilities in neuromorphic engineering"

(2019) , 9, Art.No. 4361

SCIENTIFIC REPORTS

 

175 Zhao, RD; Ma, N.; Qi, J.; Mishra, Y.K.; Adelung, R.; Yang, Y.

"Optically Controlled Abnormal Photovoltaic Current Modulation with Temperature in BiFeO3"

(2019) , 5 (3), Art.No. 1800791

ADVANCED ELECTRONIC MATERIALS

 

174 Sharma, M; Joshi, M.; Nigam, S.; Shree, S.; Avasthi, D.K.; Adelung, R.; Srivastava, S.K.; Mishra, Y.K.

"ZnO tetrapods and activated carbon based hybrid composite: Adsorbents for enhanced decontamination of hexavalent chromium from aqueous solution"

(2019) , 358, pp. 540-551

CHEMICAL ENGINEERING JOURNAL

 

173 Park, SJ; Das, G.S.; Schütt, F.; Adelung, R.; Mishra, Y.K.; Tripathi, K.M.; Kim, T.

"Visible-light photocatalysis by carbon-nano-onion-functionalized ZnO tetrapods: degradation of 2,4-dinitrophenol and a plant-model-based ecological assessment"

(2019) , 11, Art.No. 8

NPG ASIA MATERIALS

 

172 Strobel, J; Ghimpu, L.; Postica, V.; Lupan, O.; Zapf, M.; Schonherr, S.; Röder, R.; Ronning, C.; Schütt, F.; Mishra, Y.K.; Tiginyanu, I.; Adelung, R.; Marx, J.; Fiedler, B.; Kienle, L.

"Improving gas sensing by CdTe decoration of individual Aerographite microtubes"

(2019) , 30 (6), Art.No. 065501

NANOTECHNOLOGY

 

171 Taale, M; Schütt, F.; Carey, T.; Marx, J.; Mishra, Y.K.; Stock, N.; Fiedler, B.; Torrisi, F.; Adelung, R.; Selhuber-Unkel, C.

"Biomimetic Carbon Fiber Systems Engineering: A Modular Design Strategy To Generate Biofunctional Composites from Graphene and Carbon Nanofibers"

(2019) , 11 (5), pp. 5325-5335

ACS APPLIED MATERIALS & INTERFACES

 

170 Bosbach, B; Baytekin-Gerngross, M.; Sprecher, E.; Wegner, J.; Gerngross, M.D.; Carstensen, J.; Adelung, R.; Fiedler, B.

"Maximizing bearing fatigue lifetime and CAI capability of fibre metal laminates by nanoscale sculptured Al plies"

(2019) , 117, pp. 144-155

COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING

 

169 Marx, J; Roth, S.; Brouschkin, A.; Smazna, D.; Mishra, Y.K.; Schulte, K.; Adelung, R.; Fiedler, B.

"Tailored crystalline width and wall thickness of an annealed 3D carbon foam composites and their mechanical properties"

(2019) , 142, pp. 60-67

CARBON

 

168 Mintken, M; Schweichel, M.; Schröder, S.; Kaps, S.; Carstensen, J.; Mishra, Y.K.; Strunskus, T.; Faupel, F.; Adelung, R.

"Nanogenerator and piezotronic inspired concepts for energy efficient magnetic field sensors"

(2019) , 56, pp. 420-425

NANO ENERGY

 

167 Tiginyanu, I; Braniste, T.; Smazna, D.; Deng, M.; Schütt, F.; Schuchardt, A.; Stevens-Kalceff, M.A.; Raevschi, S.; Schürmann, U.; Kienle, L.; Pugno, N.M.; Mishra, Y.K.; Adelung, R.

"Self-organized and self-propelled aero-GaN with dual hydrophilic-hydrophobic behaviour"

(2019) , 56, pp. 759-769

NANO ENERGY

 

166 Song, K; Ma, N.; Mishra, Y.K.; Adelung, R.; Yang, Y.

"Achieving Light-Induced Ultrahigh Pyroelectric Charge Density Toward Self-Powered UV Light Detection"

(2019) , 5 (1), Art.No. 1800413

ADVANCED ELECTRONIC MATERIALS

 

165 Taale, M; Schütt, F.; Zheng, K.; Mishra, Y.K.; Boccaccini, A.R.; Adelung, R.; Selhuber-Unkel, C.

"Bioactive Carbon-Based Hybrid 3D Scaffolds for Osteoblast Growth"

(2018) , 10 (50), pp. 43874-43886

ACS APPLIED MATERIALS & INTERFACES

 

164 Postica, V; Vahl, A.; Strobel, J.; Santos-Carballal, D.; Lupan, O.; Cadi-Essadek, A.; de Leeuw, N.H.; Schütt, F.; Polonskyi, O.; Strunskus, T.; Baum, M.; Kienle, L.; Adelung, R.; Faupel, F.

"Tuning doping and surface functionalization of columnar oxide films for volatile organic compound sensing: experiments and theory"

(2018) , 6 (46), pp. 23669-23682

JOURNAL OF MATERIALS CHEMISTRY A

 

163 Frömling, T; Yu, R.M.; Mintken, M.; Adelung, R.; Rödel, J.

"Piezotronic sensors"

(2018) , 43 (12), pp. 941-945

MRS BULLETIN

 

162 Jiang, YT; Wang, Y.; Mishra, Y.K.; Adelung, R.; Yang, Y.

"Stretchable CNTs-Ecoflex Composite as Variable-Transmittance Skin for Ultrasensitive Strain Sensing"

(2018) , 3 (12), Art.No. 1800248

ADVANCED MATERIALS TECHNOLOGIES

 

161 Qiu, HY; Holken, I.; Gapeeva, A.; Filiz, V.; Adelung, R.; Baum, M.

"Development and Characterization of Mechanically Durable Silicone-Polythiourethane Composites Modified with Tetrapodal Shaped ZnO Particles for the Potential Application as Fouling-Release Coating in the Marine Sector"

(2018) , 11 (12), Art.No. 2413

MATERIALS

 

160 Lupan, O; Postica, V.; Ababii, N.; Reimer, T.; Shree, S.; Hoppe, M.; Polonskyi, O.; Sontea, V.; Chemnitz, S.; Faupel, F.; Adelung, R.

"Ultra-thin TiO2 films by atomic layer deposition and surface functionalization with Au nanodots for sensing applications"

(2018) , 87, pp. 44-53

MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING

 

159 Qu, MC; Terasa, M.I.; Adelung, R.; Schubert, D.W.

"Structure changes of aligned carbon nanotubes in thermoplastics below percolation revealed by impedance spectroscopy"

(2018) , 8 (8), pp. 2071-2075

APPLIED NANOSCIENCE

 

158 Bosbach, B; Baytekin-Gerngross, M.; Heyden, E.; Gerngross, M.D.; Carstensen, J.; Adelung, R.; Fiedler, B.

"Reaching maximum inter-laminar properties in GFRP/nanoscale sculptured aluminium ply laminates"

(2018) , 167, pp. 32-41

COMPOSITES SCIENCE AND TECHNOLOGY

 

157 Plesco, I; Strobel, J.; Schütt, F.; Himcinschi, C.; Ben Sedrine, N.; Monteiro, T.; Correia, M.R.; Gorceac, L.; Cinic, B.; Ursaki, V.; Marx, J.; Fiedler, B.; Mishra, Y.K.; Kienle, L.; Adelung, R.; Tiginyanu, I.

"Hierarchical Aerographite 3D flexible networks hybridized by InP micro/nanostructures for strain sensor applications"

(2018) , 8, Art.No. 13880

SCIENTIFIC REPORTS

 

156 Chauhan, N; Gupta, S.; Avasthi, D.K.; Adelung, R.; Mishra, Y.K.; Jain, U.

"Zinc Oxide Tetrapods Based Biohybrid Interface for Voltammetric Sensing of Helicobacter pylori"

(2018) , 10 (36), pp. 30631-30639

ACS APPLIED MATERIALS & INTERFACES

 

155 Demille, TB; Hughes, R.A.; Preston, A.S.; Adelung, R.; Mishra, Y.K.; Neretina, S.

"Light-Mediated Growth of Noble Metal Nanostructures (Au, Ag, Cu, Pt, Pd, Ru, Ir, Rh) From Micro- and Nanoscale ZnO Tetrapodal Backbones"

(2018) , 6, Art.No. 411

FRONTIERS IN CHEMISTRY

 

154 Pauporté, T; Lupan, O.; Postica, V.; Hoppe, M.; Chow, L.; Adelung, R.

"Al-Doped ZnO Nanowires by Electrochemical Deposition for Selective VOC Nanosensor and Nanophotodetector"

(2018) , 215 (16), Art.No. 1700824

PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE

 

153 Lupan, O; Postica, V.; Hoppe, M.; Wolff, N.; Polonskyi, O.; Pauporté, T.; Viana, B.; Majérus, O.; Kienle, L.; Faupel, F.; Adelung, R.

"PdO/PdO2 functionalized ZnO : Pd films for lower operating temperature H2 gas sensing"

(2018) , 10 (29), pp. 14107-14127

NANOSCALE

 

152 Adamski, V; Schmitt, C.; Ceynowa, F.; Adelung, R.; Lucius, R.; Synowitz, M.; Hattermann, K.; Held-Feindt, J.

"Effects of sequentially applied single and combined temozolomide, hydroxychloroquine and AT101 treatment in a long-term stimulation glioblastoma in vitro model"

(2018) , 144 (8), pp. 1475-1485

JOURNAL OF CANCER RESEARCH AND CLINICAL ONCOLOGY

 

151 Mishra, YK; Adelung, R.

"ZnO tetrapod materials for functional applications"

(2018) , 21 (6), pp. 631-651

MATERIALS TODAY

 

150 Smazna, D; Rodrigues, J.; Shree, S.; Postica, V.; Neubüser, G.; Martins, A.F.; Ben Sedrine, N.; Jena, N.K.; Siebert, L.; Schütt, F.; Lupan, O.; Ahuja, R.; Correia, M.R.; Monteiro, T.; Kienle, L.; Yang, Y.; Adelung, R.; Mishra, Y.K.

"Buckminsterfullerene hybridized zinc oxide tetrapods: defects and charge transfer induced optical and electrical response"

(2018) , 10 (21), pp. 10050-10062

NANOSCALE

 

149 Paulowicz, I; Postica, V.; Lupan, O.; Wolff, N.; Shree, S.; Cojocaru, A.; Deng, M.; Mishra, Y.K.; Tiginyanu, I.; Kienle, L.; Adelung, R.

"Zinc oxide nanotetrapods with four different arm morphologies for versatile nanosensors"

(2018) , 262, pp. 425-435

SENSORS AND ACTUATORS B-CHEMICAL

 

148 Plesco, I; Dragoman, M.; Strobel, J.; Ghimpu, L.; Schütt, F.; Dinescu, A.; Ursaki, V.; Kienle, L.; Adelung, R.; Tiginyanu, I.

"Flexible pressure sensor based on graphene aerogel microstructures functionalized with CdS nanocrystalline thin film"

(2018) , 117, pp. 418-422

SUPERLATTICES AND MICROSTRUCTURES

 

147 Qi, J; Ma, N.; Ma, X.C.; Adelung, R.; Yang, Y.

"Enhanced Photocurrent in BiFeO3 Materials by Coupling Temperature and Thermo-Phototronic Effects for Self-Powered Ultraviolet Photodetector System"

(2018) , 10 (16), pp. 13712-13719

ACS APPLIED MATERIALS & INTERFACES

 

146 Hoppe, M; Lupan, O.; Postica, V.; Wolff, N.; Duppel, V.; Kienle, L.; Tiginyanu, I.; Adelung, R.

"ZnAl2O4-Functionalized Zinc Oxide Microstructures for Highly Selective Hydrogen Gas Sensing Applications"

(2018) , 215 (7), Art.No. 1700772

PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE

 

145 Ghimpu, L; Ursaki, V.V.; Pantazi, A.; Mesterca, R.; Brâncoveanu, O.; Shree, S.; Adelung, R.; Tiginyanu, I.M.; Enachescu, M.

"Characterization of core/shell structures based on CdTe and GaAs nanocrystalline layers deposited on SnO2 microwires"

(2018) , 116, pp. 64-70

SUPERLATTICES AND MICROSTRUCTURES

 

144 Lupan, O; Wolff, N.; Postica, V.; Braniste, T.; Paulowicz, I.; Hrkac, V.; Mishra, Y.K.; Tiginyanu, I.; Kienle, L.; Adelung, R.

"Properties of a single SnO2:Zn2SnO4 - Functionalized nanowire based nanosensor"

(2018) , 44 (5), pp. 4859-4867

CERAMICS INTERNATIONAL

 

143 Hansen, S; Shree, S.; Neubüser, G.; Carstensen, J.; Kienle, L.; Adelung, R.

"Corset-like solid electrolyte interface for fast charging of silicon wire anodes"

(2018) , 381, pp. 8-17

JOURNAL OF POWER SOURCES

 

142 Hoppe, M; Ababii, N.; Postica, V.; Lupan, O.; Polonskyi, O.; Schütt, F.; Kaps, S.; Sukhodub, L.F.; Sontea, V.; Strunskus, T.; Faupel, F.; Adelung, R.

"(CuO-Cu2O)/ZnO:Al heterojunctions for volatile organic compound detection"

(2018) , 255, pp. 1362-1375

SENSORS AND ACTUATORS B-CHEMICAL

 

141 Prylepa, A; Reitböck, C.; Cobet, M.; Jesacher, A.; Jin, X.; Adelung, R.; Schatzl-Linder, M.; Luckeneder, G.; Stellnberger, K.H.; Steck, T.; Faderl, J.; Stehrer, T.; Stifter, D.

"Material characterisation with methods of nonlinear optics"

(2018) , 51 (4), Art.No. 043001

JOURNAL OF PHYSICS D-APPLIED PHYSICS

 

140 Nasajpour, A; Ansari, S.; Rinoldi, C.; Rad, A.S.; Aghaloo, T.; Shin, S.R.; Mishra, Y.K.; Adelung, R.; Swieszkowski, W.; Annabi, N.; Khademhosseini, A.; Moshaverinia, A.; Tamayol, A.

"A Multifunctional Polymeric Periodontal Membrane with Osteogenic and Antibacterial Characteristics"

(2018) , 28 (3), Art.No. 1703437

ADVANCED FUNCTIONAL MATERIALS

 

139 Schütt, F; Signetti, S.; Krüger, H.; Röder, S.; Smazna, D.; Kaps, S.; Gorb, S.N.; Mishra, Y.K.; Pugno, N.M.; Adelung, R.

"Hierarchical self-entangled carbon nanotube tube networks (vol 8, 1215, 2017)"

(2018) , 9, Art.No. 107

NATURE COMMUNICATIONS

 

138 Gerngross, MD; Baytekin-Gerngross, M.; Carstensen, J.; Adelung, R.

"Self-Organized Growth of Crystallographic Macropores in Multicrystalline Zn by Nanoscale Sculpturing"

(2018) , 165 (4), pp. H3099-H3106

JOURNAL OF THE ELECTROCHEMICAL SOCIETY

 

137 Lupan, O; Postica, V.; Adelung, R.; Labat, F.; Ciofini, I.; Schürmann, U.; Kienle, L.; Chow, L.; Viana, B.; Pauporté, T.

"Functionalized Pd/ZnO Nanowires for Nanosensors"

(2018) , 12 (1), Art.No. 1700321

PHYSICA STATUS SOLIDI-RAPID RESEARCH LETTERS

 

136 Lupan, O; Postica, V.; Labat, F.; Ciofini, I.; Pauporté, T.; Adelung, R.

"Ultra-sensitive and selective hydrogen nanosensor with fast response at room temperature based on a single Pd/ZnO nanowire"

(2018) , 254, pp. 1259-1270

SENSORS AND ACTUATORS B-CHEMICAL

 

135 Marx, J; Brouschkin, A.; Roth, S.; Smazna, D.; Mishra, Y.K.; Wittich, H.; Schulte, K.; Adelung, R.; Fiedler, B.

"Fundamentals of the temperature-dependent electrical conductivity of a 3D carbon foam-Aerographite"

(2018) , 235, pp. 145-152

SYNTHETIC METALS

 

134 Gröttrup, J; Postica, V.; Smazna, D.; Hoppe, M.; Kaidas, V.; Mishra, Y.K.; Lupan, O.; Adelung, R.

"UV detection properties of hybrid ZnO tetrapod 3-D networks"

(2017) , 146, pp. 492-500

VACUUM

 

133 Gröttrup, J; Schütt, F.; Smazna, D.; Lupan, O.; Adelung, R.; Mishra, Y.K.

"Porous ceramics based on hybrid inorganic tetrapodal networks for efficient photocatalysis and water purification"

(2017) , 43 (17), pp. 14915-14922

CERAMICS INTERNATIONAL

 

132 Kallweit, C; Bremer, M.; Smazna, D.; Karrock, T.; Adelung, R.; Gerken, M.

"Photoresponsive hierarchical ZnO-PDMS surfaces with azobenzene-polydopamine coated nanoparticles for reversible wettability tuning"

(2017) , 146, pp. 386-395

VACUUM

 

131 Lupan, O; Schütt, F.; Postica, V.; Smazna, D.; Mishra, Y.K.; Adelung, R.

"Sensing performances of pure and hybridized carbon nanotubes-ZnO nanowire networks: A detailed study"

(2017) , 7, Art.No. 14715

SCIENTIFIC REPORTS

 

130 Neubüser, G; Hansen, S.; Duppel, V.; Adelung, R.; Kienle, L.

"(Re-)crystallization mechanism of highly oriented Si-microwire arrays by TEM analysis"

(2017) , 21 (12), pp. 3421-3427

JOURNAL OF SOLID STATE ELECTROCHEMISTRY

 

129 Schürmann, U; Chluba, C.; Wolff, N.; Smazna, D.; de Miranda, R.L.; Junker, P.; Adelung, R.; Quandt, E.; Kienle, L.

"Functional NiTi grids for in situ straining in the TEM"

(2017) , 182, pp. 10-16

ULTRAMICROSCOPY

 

128 Shree, S; Schulz-Senft, M.; Alsleben, N.H.; Mishra, Y.K.; Staubitz, A.; Adelung, R.

"Light, Force, and Heat: A Multi-Stimuli Composite that Reveals its Violent Past"

(2017) , 9 (43), pp. 38000-38007

ACS APPLIED MATERIALS & INTERFACES

 

127 Schütt, F; Signetti, S.; Krüger, H.; Röder, S.; Smazna, D.; Kaps, S.; Gorb, S.N.; Mishra, Y.K.; Pugno, N.M.; Adelung, R.

"Hierarchical self-entangled carbon nanotube tube networks"

(2017) , 8, Art.No. 1215

NATURE COMMUNICATIONS

 

126 Postica, V; Schtt, F.; Adelung, R.; Lupan, O.

"Schottky Diode Based on a Single Carbon-Nanotube-ZnO Hybrid Tetrapod for Selective Sensing Applications"

(2017) , 4 (19), Art.No. 1700507

ADVANCED MATERIALS INTERFACES

 

125 Faraji, N; Adelung, R.; Mishra, Y.K.; Seidel, J.

"Nanoscale electromechanical and electronic properties of free-standing ZnO nano- and microstructured platelets"

(2017) , 28 (40), Art.No. 405701

NANOTECHNOLOGY

 

124 Nasajpour, A; Mandla, S.; Shree, S.; Mostafavi, E.; Sharifi, R.; Khalilpour, A.; Saghazadeh, S.; Hassan, S.; Mitchell, M.J.; Leijten, J.; Hou, X.; Moshaverinia, A.; Annabi, N.; Adelung, R.; Mishra, Y.K.; Shin, S.R.; Tamayol, A.; Khademhosseini, A.

"Nanostructured Fibrous Membranes with Rose Spike-Like Architecture"

(2017) , 17 (10), pp. 6235-6240

NANO LETTERS

 

123 Postica, V; Hoppe, M.; Gröttrup, J.; Hayes, P.; Röbisch, V.; Smazna, D.; Adelung, R.; Viana, B.; Aschehoug, P.; Pauporté, T.; Lupan, O.

"Morphology dependent UV photoresponse of Sn-doped ZnO microstructures"

(2017) , 71, pp. 75-86

SOLID STATE SCIENCES

 

122 Hrkac, SB; Koops, C.T.; Abes, M.; Krywka, C.; Müller, M.; Burghammer, M.; Sztucki, M.; Dane, T.; Kaps, S.; Mishra, Y.K.; Adelung, R.; Schmalz, J.; Gerken, M.; Lage, E.; Kirchhof, C.; Quandt, E.; Magnussen, O.M.; Murphy, B.M.

"Tunable Strain in Magnetoelectric ZnO Microrod Composite Interfaces"

(2017) , 9 (30), pp. 25571-25577

ACS APPLIED MATERIALS & INTERFACES

 

121 Schütt, F; Postica, V.; Adelung, R.; Lupan, O.

"Single and Networked ZnO-CNT Hybrid Tetrapods for Selective Room-Temperature High-Performance Ammonia Sensors"

(2017) , 9 (27), pp. 23107-23118

ACS APPLIED MATERIALS & INTERFACES

 

120 Lupan, O; Postica, V.; Marx, J.; Mecklenburg, M.; Mishra, Y.K.; Schulte, K.; Fiedler, B.; Adelung, R.

"Individual hollow and mesoporous aero-graphitic microtube based devices for gas sensing applications"

(2017) , 110 (26), Art.No. 263109

APPLIED PHYSICS LETTERS

 

119 Kaps, S; Bhowmick, S.; Gröttrup, J.; Hrkac, V.; Stauffer, D.; Guo, H.; Warren, O.L.; Adam, J.; Kienle, L.; Minor, A.M.; Adelung, R.; Mishra, Y.K.

"Piezoresistive Response of Quasi-One-Dimensional ZnO Nanowires Using an in Situ Electromechanical Device"

(2017) , 2 (6), pp. 2985-2993

ACS OMEGA

 

118 Lupan, O; Postica, V.; Gröttrup, J.; Mishra, A.K.; de Leeuw, N.H.; Adelung, R.

"Enhanced UV and ethanol vapour sensing of a single 3-D ZnO tetrapod alloyed with Fe2O3 nanoparticles"

(2017) , 245, pp. 448-461

SENSORS AND ACTUATORS B-CHEMICAL

 

117 Silva, EL; Mishra, Y.K.; Fernandes, A.J.S.; Silva, R.F.; Strobel, J.; Kienle, L.; Adelung, R.; Oliveira, F.J.; Zheludkevich, M.L.

"Direct Synthesis of Electrowettable Carbon Nanowall-Diamond Hybrid Materials from Sacrificial Ceramic Templates Using HFCVD"

(2017) , 4 (10), Art.No. 1700019

ADVANCED MATERIALS INTERFACES

 

116 Hansen, S; Quiroga-González, E.; Carstensen, J.; Adelung, R.; Föll, H.

"Size-dependent physicochemical and mechanical interactions in battery paste anodes of Si-microwires revealed by Fast-Fourier-Transform Impedance Spectroscopy"

(2017) , 349, pp. 1-10

JOURNAL OF POWER SOURCES

 

115 Lupan, O; Postica, V.; Wolff, N.; Polonskyi, O.; Duppel, V.; Kaidas, V.; Lazari, E.; Ababii, N.; Faupel, F.; Kienle, L.; Adelung, R.

"Localized Synthesis of Iron Oxide Nanowires and Fabrication of High Performance Nanosensors Based on a Single Fe2O3 Nanowire"

(2017) , 13 (16), Art.No. 1602868

SMALL

 

114 Gröttrup, J; Postica, V.; Ababii, N.; Lupan, O.; Zamponi, C.; Meyners, D.; Mishra, Y.K.; Sontea, V.; Tiginyanu, I.; Adelung, R.

"Size-dependent UV and gas sensing response of individual Fe2O3-ZnO:Fe micro- and nanowire based devices"

(2017) , 701, pp. 920-925

JOURNAL OF ALLOYS AND COMPOUNDS

 

113 Meija, R; Signetti, S.; Schuchardt, A.; Meurisch, K.; Smazna, D.; Mecklenburg, M.; Schulte, K.; Erts, D.; Lupan, O.; Fiedler, B.; Mishra, Y.K.; Adelung, R.; Pugno, N.M.

"Nanomechanics of individual aerographite tetrapods"

(2017) , 8, Art.No. 14982

NATURE COMMUNICATIONS

 

112 Parlak, O; Mishra, Y.K.; Grigoriev, A.; Mecklenburg, M.; Luo, W.; Keene, S.; Salleo, A.; Schulte, K.; Ahuja, R.; Adelung, R.; Turner, A.P.F.; Tiwari, A.

"Hierarchical Aerographite nano-microtubular tetrapodal networks based electrodes as lightweight supercapacitor"

(2017) , 34, pp. 570-577

NANO ENERGY

 

111 Duggal, N; Jaishankar, D.; Yadavalli, T.; Hadigal, S.; Mishra, Y.K.; Adelung, R.; Shukla, D.

"Zinc oxide tetrapods inhibit herpes simplex virus infection of cultured corneas"

(2017) , 23, pp. 26-38

MOLECULAR VISION

 

110 Postica, V; Gröttrup, J.; Adelung, R.; Lupan, O.; Mishra, A.K.; de Leeuw, N.H.; Ababii, N.; Carreira, J.F.C.; Rodrigues, J.; Ben Sedrine, N.; Correia, M.R.; Monteiro, T.; Sontea, V.; Mishra, Y.K.

"Multifunctional Materials: A Case Study of the Effects of Metal Doping on ZnO Tetrapods with Bismuth and Tin Oxides"

(2017) , 27 (6), Art.No. 1604676

ADVANCED FUNCTIONAL MATERIALS

 

109 Lupan, O; Postica, V.; Gröttrup, J.; Mishra, A.K.; de Leeuw, N.H.; Carreira, J.F.C.; Rodrigues, J.; Ben Sedrine, N.; Correia, M.R.; Monteiro, T.; Cretu, V.; Tiginyanu, I.; Smazna, D.; Mishra, Y.K.; Adelung, R.

"Hybridization of Zinc Oxide Tetrapods for Selective Gas Sensing Applications"

(2017) , 9 (4), pp. 4084-4099

ACS APPLIED MATERIALS & INTERFACES

 

108 Garlof, S; Mecklenburg, M.; Smazna, D.; Mishra, Y.K.; Adelung, R.; Schulte, K.; Fiedler, B.

"3D carbon networks and their polymer composites: Fabrication and electromechanical investigations of neat Aerographite and Aerographite-based PNCs under compressive load"

(2017) , 111, pp. 103-112

CARBON

 

107 Garlof, S; Fukuda, T.; Mecklenburg, M.; Smazna, D.; Mishra, Y.K.; Adelung, R.; Schulte, K.; Fiedler, B.

"Electro-mechanical piezoresistive properties of three dimensionally interconnected carbon aerogel (Aerographite)-epoxy composites"

(2016) , 134, pp. 226-233

COMPOSITES SCIENCE AND TECHNOLOGY

 

106 Lupan, O; Postica, V.; Ababii, N.; Hoppe, M.; Cretu, V.; Tiginyanu, I.; Sontea, V.; Pauporté, T.; Viana, B.; Adelung, R.

"Influence of CuO nanostructures morphology on hydrogen gas sensing performances"

(2016) , 164, pp. 63-70

MICROELECTRONIC ENGINEERING

 

105 Tiginyanu, I; Ghimpu, L.; Gröttrup, J.; Postolache, V.; Mecklenburg, M.; Stevens-Kalceff, M.A.; Ursaki, V.; Payami, N.; Feidenhansl, R.; Schulte, K.; Adelung, R.; Mishra, Y.K.

"Strong light scattering and broadband (UV to IR) photoabsorption in stretchable 3D hybrid architectures based on Aerographite decorated by ZnO nanocrystallites"

(2016) , 6, Art.No. 32913

SCIENTIFIC REPORTS

 

104 Faraji, N; Ulrich, C.; Wolff, N.; Kienle, L.; Adelung, R.; Mishra, Y.K.; Seidel, J.

"Visible-Light Driven Nanoscale Photoconductivity of Grain Boundaries in Self-Supported ZnO Nano- and Microstructured Platelets"

(2016) , 2 (9), Art.No. 1600138

ADVANCED ELECTRONIC MATERIALS

 

103 Wille, S; Hölken, I.; Haidarschin, G.; Adelung, R.; Kern, M.

"Biaxial flexural strength of new Bis-GMA/TEGDMA based composites with different fillers for dental applications"

(2016) , 32 (9), pp. 1073-1078

DENTAL MATERIALS

 

102 Hölken, I; Neubüser, G.; Postica, V.; Bumke, L.; Lupan, O.; Baum, M.; Mishra, Y.K.; Kienle, L.; Adelung, R.

"Sacrificial Template Synthesis and Properties of 3D Hollow-Silicon Nano- and Microstructures"

(2016) , 8 (31), pp. 20491-20498

ACS APPLIED MATERIALS & INTERFACES

 

101 Gröttrup, J; Kaps, S.; Carstensen, J.; Smazna, D.; Mishra, Y.K.; Piorra, A.; Kirchhof, C.; Quandt, E.; Adelung, R.

"Piezotronic-based magnetoelectric sensor: Fabrication and response"

(2016) , 213 (8), pp. 2208-2215

PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE

 

100 Lupan, O; Cretu, V.; Postica, V.; Polonskyi, O.; Ababii, N.; Schütt, F.; Kaidas, V.; Faupel, F.; Adelung, R.

"Non-planar nanoscale p-p heterojunctions formation in ZnxCu1-xOy nanocrystals by mixed phases for enhanced sensors"

(2016) , 230, pp. 832-843

SENSORS AND ACTUATORS B-CHEMICAL

 

99 Postica, V; Hölken, I.; Schneider, V.; Kaidas, V.; Polonskyi, O.; Cretu, V.; Tiginyanu, I.; Faupel, F.; Adelung, R.; Lupan, O.

"Multifunctional device based on ZnO:Fe nanostructured films with enhanced UV and ultra-fast ethanol vapour sensing"

(2016) , 49, pp. 20-33

MATERIALS SCIENCE IN SEMICONDUCTOR PROCESSING

 

98 Lamprecht, C; Taale, M.; Paulowicz, I.; Westerhaus, H.; Grabosch, C.; Schuchardt, A.; Mecklenburg, M.; Böttner, M.; Lucius, R.; Schulte, K.; Adelung, R.; Selhuber-Unkel, C.

"A Tunable Scaffold of Microtubular Graphite for 3D Cell Growth"

(2016) , 8 (24), pp. 14980-14985

ACS APPLIED MATERIALS & INTERFACES

 

97 Antoine, TE; Hadigal, S.R.; Yakoub, A.M.; Mishra, Y.K.; Bhattacharya, P.; Haddad, C.; Valyi-Nagy, T.; Adelung, R.; Prabhakar, B.S.; Shukla, D.

"Intravaginal Zinc Oxide Tetrapod Nanoparticles as Novel Immunoprotective Agents against Genital Herpes"

(2016) , 196 (11), pp. 4566-4575

JOURNAL OF IMMUNOLOGY

 

96 Gröttrup, J; Paulowicz, I.; Schuchardt, A.; Kaidas, V.; Kaps, S.; Lupan, O.; Adelung, R.; Mishra, Y.K.

"Three-dimensional flexible ceramics based on interconnected network of highly porous pure and metal alloyed ZnO tetrapods"

(2016) , 42 (7), pp. 8664-8676

CERAMICS INTERNATIONAL

 

95 Kizilkan, E; Strueben, J.; Jin, X.; Schaber, C.F.; Adelung, R.; Staubitz, A.; Gorb, S.N.

"Influence of the porosity on the photoresponse of a liquid crystal elastomer"

(2016) , 3 (4), Art.No. 150700

ROYAL SOCIETY OPEN SCIENCE

 

94 Hölken, I; Hoppe, M.; Mishra, Y.K.; Gorb, S.N.; Adelung, R.; Baum, M.J.

"Complex shaped ZnO nano- and microstructure based polymer composites: mechanically stable and environmentally friendly coatings for potential antifouling applications"

(2016) , 18 (10), pp. 7114-7123

PHYSICAL CHEMISTRY CHEMICAL PHYSICS

 

93 Lupan, O; Postica, V.; Cretu, V.; Wolff, N.; Duppel, V.; Kienle, L.; Adelung, R.

"Single and networked CuO nanowires for highly sensitive p-type semiconductor gas sensor applications"

(2016) , 10 (3), pp. 260-266

PHYSICA STATUS SOLIDI-RAPID RESEARCH LETTERS

 

92 Lupan, O; Cretu, V.; Postica, V.; Ababii, N.; Polonskyi, O.; Kaidas, V.; Schut, F.; Mishra, Y.K.; Monaico, E.; Tiginyanu, I.; Sontea, V.; Strunskus, T.; Faupel, F.; Adelung, R.

"Enhanced ethanol vapour sensing performances of copper oxide nanocrystals with mixed phases"

(2016) , 224, pp. 434-448

SENSORS AND ACTUATORS B-CHEMICAL

 

91 Lupan, O; Cretu, V.; Postica, V.; Ahmadi, M.; Roldan Cuenya, B.; Chow, L.; Tiginyanu, I.; Viana, B.; Pauporté, T.; Adelung, R.

"Silver-doped zinc oxide single nanowire multifunctional nanosensor with a significant enhancement in response"

(2016) , 223, pp. 893-903

SENSORS AND ACTUATORS B-CHEMICAL

 

90 Chandrasekaran, S; Liebig, W.V.; Mecklenburg, M.; Fiedler, B.; Smazna, D.; Adelung, R.; Schulte, K.

"Fracture, failure and compression behaviour of a 3D interconnected carbon aerogel (Aerographite) epoxy composite"

(2016) , 122, pp. 50-58

COMPOSITES SCIENCE AND TECHNOLOGY

 

89 Baytekin-Gerngross, M; Gerngross, M.D.; Carstensen, J.; Adelung, R.

"Making metal surfaces strong, resistant, and multifunctional by nanoscale-sculpturing"

(2016) , 1 (6), pp. 467-472

NANOSCALE HORIZONS

 

88 Cretu, V; Postica, V.; Mishra, A.K.; Hoppe, M.; Tiginyanu, I.; Mishra, Y.K.; Chow, L.; de Leeuw, N.H.; Adelung, R.; Lupan, O.

"Synthesis, characterization and DFT studies of zinc-doped copper oxide nanocrystals for gas sensing applications"

(2016) , 4 (17), pp. 6527-6539

JOURNAL OF MATERIALS CHEMISTRY A

 

87 Gerngross, MD; Carstensen, J.; Föll, H.; Adelung, R.

"FFT-impedance spectroscopy analysis of the growth of magnetic metal nanowires in ultra-high aspect ratio InP membranes"

(2016) , 31 (1), Art.No. 014005

SEMICONDUCTOR SCIENCE AND TECHNOLOGY

 

86 Hansen, S; Schütt, A.; Carstensen, J.; Adelung, R.

"Local Transmittance Measurements as Large Area Diagnostic Tool for the Optimization of Porous Si Foils for Li-Ion Battery Anodes"

(2016) , 163 (14), pp. A3036-A3045

JOURNAL OF THE ELECTROCHEMICAL SOCIETY

 

85 Lupan, O; Postica, V.; Mecklenburg, M.; Schulte, K.; Mishra, Y.K.; Fiedler, B.; Adelung, R.

"Low powered, tunable and ultra-light aerographite sensor for climate relevant gas monitoring"

(2016) , 4 (42), pp. 16723-16730

JOURNAL OF MATERIALS CHEMISTRY A

 

84 Tiginyanu, I; Stevens-Kalceff, M.A.; Sarua, A.; Braniste, T.; Monaico, E.; Popa, V.; Andrade, H.D.; Thomas, J.O.; Raevschi, S.; Schulte, K.; Adelung, R.

"Self-Organized Three-Dimensional Nanostructured Architectures in Bulk GaN Generated by Spatial Modulation of Doping"

(2016) , 5 (5), pp. P218-P227

ECS JOURNAL OF SOLID STATE SCIENCE AND TECHNOLOGY

 

83 Lupan, O; Braniste, T.; Deng, M.; Ghimpu, L.; Paulowicz, I.; Mishra, Y.K.; Kienle, L.; Adelung, R.; Tiginyanu, I.

"Rapid switching and ultra-responsive nanosensors based on individual shell core Ga2O3/GaN:Ox@SnO2 nanobelt with nanocrystalline shell in mixed phases"

(2015) , 221, pp. 544-555

SENSORS AND ACTUATORS B-CHEMICAL

 

82 Paulowicz, I; Hrkac, V.; Kaps, S.; Cretu, V.; Lupan, O.; Braniste, T.; Duppel, V.; Tiginyanu, I.; Kienle, L.; Adelung, R.; Mishra, Y.K.

"Three-Dimensional SnO2 Nanowire Networks for Multifunctional Applications: From High-Temperature Stretchable Ceramics to Ultraresponsive Sensors"

(2015) , 1 (8), Art.No. 1500081

ADVANCED ELECTRONIC MATERIALS

 

81 Mishra, YK; Modi, G.; Cretu, V.; Postica, V.; Lupan, O.; Reimer, T.; Paulowicz, I.; Hrkac, V.; Benecke, W.; Kienle, L.; Adelung, R.

"Direct Growth of Freestanding ZnO Tetrapod Networks for Multifunctional Applications in Photocatalysis, UV Photodetection, and Gas Sensing"

(2015) , 7 (26), pp. 14303-14316

ACS APPLIED MATERIALS & INTERFACES

 

80 Schuchardt, A; Braniste, T.; Mishra, Y.K.; Deng, M.; Mecklenburg, M.; Stevens-Kalceff, M.A.; Raevschi, S.; Schulte, K.; Kienle, L.; Adelung, R.; Tiginyanu, I.

"Three-dimensional Aerographite-GaN hybrid networks: Single step fabrication of porous and mechanically flexible materials for multifunctional applications"

(2015) , 5, Art.No. 8839

SCIENTIFIC REPORTS

 

79 Enachi, M; Lupan, O.; Braniste, T.; Sarua, A.; Chow, L.; Mishra, Y.K.; Gedamu, D.; Adelung, R.; Tiginyanu, I.

"Integration of individual TiO2 nanotube on the chip: Nanodevice for hydrogen sensing"

(2015) , 9 (3), pp. 171-174

PHYSICA STATUS SOLIDI-RAPID RESEARCH LETTERS

 

78 Monaico, E; Postolache, V.; Borodin, E.; Ursaki, V.V.; Lupan, O.; Adelung, R.; Nielsch, K.; Tiginyanu, I.M.

"Control of persistent photoconductivity in nanostructured InP through morphology design"

(2015) , 30 (3), Art.No. 035014

SEMICONDUCTOR SCIENCE AND TECHNOLOGY

 

77 Najim, M; Modi, G.; Mishra, Y.K.; Adelung, R.; Singh, D.; Agarwala, V.

"Ultra-wide bandwidth with enhanced microwave absorption of electroless Ni-P coated tetrapod-shaped ZnO nano- and microstructures"

(2015) , 17 (35), pp. 22923-22933

PHYSICAL CHEMISTRY CHEMICAL PHYSICS

 

76 Jin, X; Deng, M.; Kaps, S.R.; Zhu, X.W.; Hölken, I.; Mess, K.; Adelung, R.; Mishra, Y.K.

"Study of Tetrapodal ZnO-PDMS Composites: A Comparison of Fillers Shapes in Stiffness and Hydrophobicity Improvements"

(2014) , 9 (9), Art.No. e106991

PLOS ONE

 

75 Jin, X; Heepe, L.; Strueben, J.; Adelung, R.; Gorb, S.N.; Staubitz, A.

"Challenges and Solutions for Joining Polymer Materials"

(2014) , 35 (18), pp. 1551-1570

MACROMOLECULAR RAPID COMMUNICATIONS

 

74 Jahns, R; Zabel, S.; Marauska, S.; Gojdka, B.; Wagner, B.; Knöchel, R.; Adelung, R.; Faupel, F.

"Microelectromechanical magnetic field sensor based on ΔE effect"

(2014) , 105 (5), Art.No. 052414

APPLIED PHYSICS LETTERS

 

73 Lupan, O; Cretu, V.; Deng, M.; Gedamu, D.; Paulowicz, I.; Kaps, S.; Mishra, Y.K.; Polonskyi, O.; Zamponi, C.; Kienle, L.; Trofim, V.; Tiginyanu, I.; Adelung, R.

"Versatile Growth of Freestanding Orthorhombic α-Molybdenum Trioxide Nano- and Microstructures by Rapid Thermal Processing for Gas Nanosensors"

(2014) , 118 (27), pp. 15068-15078

JOURNAL OF PHYSICAL CHEMISTRY C

 

72 Reimer, T; Paulowicz, I.; Röder, R.; Kaps, S.; Lupan, O.; Chemnitz, S.; Benecke, W.; Ronning, C.; Adelung, R.; Mishra, Y.K.

"Single Step Integration of ZnO Nano- and Microneedles in Si Trenches by Novel Flame Transport Approach: Whispering Gallery Modes and Photocatalytic Properties"

(2014) , 6 (10), pp. 7806-7815

ACS APPLIED MATERIALS & INTERFACES

 

71 Gedamu, D; Lupan, O.; Mishra, Y.K.; Adelung, R.

"Integration of Metal and Metal Oxide Nanowires Directly on Chip by Top-Down Technology and Their Electrical Characteristics"

(2014) , 9 (2), pp. 239-246

JOURNAL OF NANOELECTRONICS AND OPTOELECTRONICS

 

70 Lupan, O; Ghimpu, L.; Reimer, T.; Hoppe, M.; Paulowicz, I.; Gedamu, D.; Mishra, Y.K.; Hammerich, D.; Chemnitz, S.; Cretu, V.; Tiginyanu, I.; Adelung, R.

"Magnetron Sputtering and Characterization of Doped Zinc Oxide Nanofibrous Films and Their Applications"

(2014) , 9 (2), pp. 257-264

JOURNAL OF NANOELECTRONICS AND OPTOELECTRONICS

 

69 Tiginyanu, I; Adelung, R.

"A Special Section on Nanotechnologies and Nanomaterials for Electronic and Photonic Applications"

(2014) , 9 (2), pp. 193-195

JOURNAL OF NANOELECTRONICS AND OPTOELECTRONICS

 

68 Gedamu, D; Paulowicz, I.; Kaps, S.; Lupan, O.; Wille, S.; Haidarschin, G.; Mishra, Y.K.; Adelung, R.

"Rapid Fabrication Technique for Interpenetrated ZnO Nanotetrapod Networks for Fast UV Sensors"

(2014) , 26 (10), pp. 1541-1550

ADVANCED MATERIALS

 

67 Lupan, O; Trofim, V.; Cretu, V.; Stamov, I.; Syrbu, N.N.; Tiginyanu, I.; Mishra, Y.K.; Adelung, R.

"Investigation of optical properties and electronic transitions in bulk and nano-microribbons of molybdenum trioxide"

(2014) , 47 (8), Art.No. 085302

JOURNAL OF PHYSICS D-APPLIED PHYSICS

 

66 Papavlassopoulos, H; Mishra, Y.K.; Kaps, S.; Paulowicz, I.; Abdelaziz, R.; Elbahri, M.; Maser, E.; Adelung, R.; Röhl, C.

"Impact of cell culture and particle parameters on the toxicity of zinc oxide nano-micro structures in vitro to fibroblasts"

(2014) , 387, pp. S73-S73

NAUNYN-SCHMIEDEBERGS ARCHIVES OF PHARMACOLOGY

 

65 Papavlassopoulos, H; Mishra, Y.K.; Kaps, S.; Paulowicz, I.; Abdelaziz, R.; Elbahri, M.; Maser, E.; Adelung, R.; Röhl, C.

"Toxicity of Functional Nano-Micro Zinc Oxide Tetrapods: Impact of Cell Culture Conditions, Cellular Age and Material Properties"

(2014) , 9 (1), Art.No. e84983

PLOS ONE

 

64 Mishra, YK; Kaps, S.; Schuchardt, A.; Paulowicz, I.; Jin, X.; Gedamu, D.; Wille, S.; Lupan, O.; Adelung, R.

"Versatile Fabrication of Complex Shaped Metal Oxide Nano-Microstructures and Their Interconnected Networks for Multifunctional Applications"

(2014) (31), pp. 92-110

KONA POWDER AND PARTICLE JOURNAL

 

63 Hrkac, SB; Abes, M.; Koops, C.T.; Krywka, C.; Müller, M.; Kaps, S.; Adelung, R.; McCord, J.; Lage, E.; Quandt, E.; Magnussen, O.M.; Murphy, B.M.

"Local magnetization and strain in single magnetoelectric microrod composites"

(2013) , 103 (12), Art.No. 123111

APPLIED PHYSICS LETTERS

 

62 Mishra, YK; Kaps, S.; Schuchardt, A.; Paulowicz, I.; Jin, X.; Gedamu, D.; Freitag, S.; Claus, M.; Wille, S.; Kovalev, A.; Gorb, S.N.; Adelung, R.

"Fabrication of Macroscopically Flexible and Highly Porous 3D Semiconductor Networks from Interpenetrating Nanostructures by a Simple Flame Transport Approach"

(2013) , 30 (9), pp. 775-783

PARTICLE & PARTICLE SYSTEMS CHARACTERIZATION

 

61 Mishra, YK; Adelung, R.; Kumar, G.; Elbahri, M.; Mohapatra, S.; Singhal, R.; Tripathi, A.; Avasthi, D.K.

"Formation of Self-organized Silver Nanocup-Type Structures and Their Plasmonic Absorption"

(2013) , 8 (2), pp. 811-815

PLASMONICS

 

60 Hrkac, V; Kienle, L.; Kaps, S.; Lotnyk, A.; Mishra, Y.K.; Schürmann, U.; Duppel, V.; Lotsch, B.V.; Adelung, R.

"Superposition twinning supported by texture in ZnO nanospikes"

(2013) , 46, pp. 396-403

JOURNAL OF APPLIED CRYSTALLOGRAPHY

 

59 Jin, X; Götz, M.; Wille, S.; Mishra, Y.K.; Adelung, R.; Zollfrank, C.

"A Novel Concept for Self-Reporting Materials: Stress Sensitive Photoluminescence in ZnO Tetrapod Filled Elastomers"

(2013) , 25 (9), pp. 1342-1347

ADVANCED MATERIALS

 

58 Tiginyanu, IM; Volciuc, O.; Stevens-Kalceff, M.A.; Popa, V.; Gutowski, J.; Wille, S.; Adelung, R.; Föll, H.

"The impact of the discreteness of low-fluence ion beam processing on the spatial architecture of GaN nanostructures fabricated by surface charge lithography"

(2013) , 49 (1), pp. 1-3

SURFACE ENGINEERING AND APPLIED ELECTROCHEMISTRY

 

57 Antoine, TE; Mishra, Y.K.; Trigilio, J.; Tiwari, V.; Adelung, R.; Shukla, D.

"Prophylactic, therapeutic and neutralizing effects of zinc oxide tetrapod structures against herpes simplex virus type-2 infection"

(2012) , 96 (3), pp. 363-375

ANTIVIRAL RESEARCH

 

56 Jin, X; Strueben, J.; Heepe, L.; Kovalev, A.; Mishra, Y.K.; Adelung, R.; Gorb, S.N.; Staubitz, A.

"Joining the Un-Joinable: Adhesion Between Low Surface Energy Polymers Using Tetrapodal ZnO Linkers"

(2012) , 24 (42), pp. 5676-5680

ADVANCED MATERIALS

 

55 Trigilio, J; Antoine, T.E.; Paulowicz, I.; Mishra, Y.K.; Adelung, R.; Shukla, D.

"Tin Oxide Nanowires Suppress Herpes Simplex Virus-1 Entry and Cell-to-Cell Membrane Fusion"

(2012) , 7 (10), Art.No. e48147

PLOS ONE

 

54 Mishra, YK; Chakravadhanula, V.S.K.; Hrkac, V.; Jebril, S.; Agarwal, D.C.; Mohapatra, S.; Avasthi, D.K.; Kienle, L.; Adelung, R.

"Crystal growth behaviour in Au-ZnO nanocomposite under different annealing environments and photoswitchability"

(2012) , 112 (6), Art.No. 064308

JOURNAL OF APPLIED PHYSICS

 

53 Zarie, ES; Kaidas, V.; Gedamu, D.; Mishra, Y.K.; Adelung, R.; Furkert, F.H.; Scherliess, R.; Steckel, H.; Groessner-Schreiber, B.

"Solvent Free Fabrication of Micro and Nanostructured Drug Coatings by Thermal Evaporation for Controlled Release and Increased Effects"

(2012) , 7 (8), Art.No. e40746

PLOS ONE

 

52 Mecklenburg, M; Schuchardt, A.; Mishra, Y.K.; Kaps, S.; Adelung, R.; Lotnyk, A.; Kienle, L.; Schulte, K.

"Aerographite: Ultra Lightweight, Flexible Nanowall, Carbon Microtube Material with Outstanding Mechanical Performance"

(2012) , 24 (26), pp. 3486-3490

ADVANCED MATERIALS

 

51 Sayed, FN; Jayakumar, O.D.; Sasikala, R.; Kadam, R.M.; Bharadwaj, S.R.; Kienle, L.; Schürmann, U.; Kaps, S.; Adelung, R.; Mittal, J.P.; Tyagi, A.K.

"Photochemical Hydrogen Generation Using Nitrogen-Doped TiO2-Pd Nanoparticles: Facile Synthesis and Effect of Ti3+ Incorporation"

(2012) , 116 (23), pp. 12462-12467

JOURNAL OF PHYSICAL CHEMISTRY C

 

50 Gojdka, B; Jahns, R.; Meurisch, K.; Greve, H.; Adelung, R.; Quandt, E.; Knöchel, R.; Faupel, F.

"Fully integrable magnetic field sensor based on delta-E effect"

(2011) , 99 (22), Art.No. 223502

APPLIED PHYSICS LETTERS

 

49 Mishra, YK; Adelung, R.; Röhl, C.; Shukla, D.; Spors, F.; Tiwari, V.

"Virostatic potential of micro-nano filopodia-like ZnO structures against herpes simplex virus-1"

(2011) , 92 (2), pp. 305-312

ANTIVIRAL RESEARCH

 

48 Gedamu, D; Jebril, S.; Schuchardt, A.; Elbahri, M.; Wille, S.; Mishra, Y.K.; Adelung, R.

"Examples for the integration of self-organized nanowires for functional devices by a fracture approach"

(2010) , 247 (10), pp. 2571-2580

PHYSICA STATUS SOLIDI B-BASIC SOLID STATE PHYSICS

 

47 Jebril, S; Kuhlmann, H.; Müller, S.; Ronning, C.; Kienle, L.; Duppel, V.; Mishra, Y.K.; Adelung, R.

"Epitactically Interpenetrated High Quality ZnO Nanostructured Junctions on Microchips Grown by the Vapor-Liquid-Solid Method"

(2010) , 10 (7), pp. 2842-2846

CRYSTAL GROWTH & DESIGN

 

46 Rätzke, K; Wiegemann, M.; Shaikh, M.Q.; Harms, S.; Adelung, R.; Egger, W.; Sperr, P.

"Open volume in bioadhesive detected by positron annihilation lifetime spectroscopy"

(2010) , 6 (7), pp. 2690-2694

ACTA BIOMATERIALIA

 

45 Nemcsics, A; Nagy, S.; Mojzes, I.; Schwedhelm, R.; Woedtke, S.; Adelung, R.; Kipp, L.

"Investigation of the surface morphology on epitaxially grown fullerene structures"

(2009) , 84 (1), pp. 152-154

VACUUM

 

44 Jebril, S; Elbahri, M.; Titazu, G.; Subannajui, K.; Essa, S.; Niebelschütz, F.; Röhlig, C.C.; Cimalla, V.; Ambacher, O.; Schmidt, B.; Kabiraj, D.; Avasti, D.; Adelung, R.

"Integration of Thin-Film-Fracture-Based Nanowires into Microchip Fabrication"

(2008) , 4 (12), pp. 2214-2221

SMALL

 

43 Wichmann, MHG; Buschhorn, S.T.; Böger, L.; Adelung, R.; Schulte, K.

"Direction sensitive bending sensors based on multi-wall carbon nanotube/epoxy nanocomposites"

(2008) , 19 (47), Art.No. 475503

NANOTECHNOLOGY

 

42 Prehn, K; Adelung, R.; Heinen, M.; Nunes, S.P.; Schulte, K.

"Catalytically active CNT-polymer-membrane assemblies: From synthesis to application"

(2008) , 321 (1), pp. 123-130

JOURNAL OF MEMBRANE SCIENCE

 

41 Takele, H; Jebril, S.; Strunskus, T.; Zaporojchenko, V.; Adelung, R.; Faupel, F.

"Tuning of electrical and structural properties of metal-polymer nanocomposite films prepared by co-evaporation technique"

(2008) , 92 (2), pp. 345-350

APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING

 

40 Hallmann, L; Bashir, A.; Strunskus, T.; Adelung, R.; Staemmler, V.; Wöll, C.; Tuczek, F.

"Self-assembled monolayers of benzylmercaptan and p-cyanobenzylmereaptan on Au(111) surfaces:: Structural and spectroscopic characterization"

(2008) , 24 (11), pp. 5726-5733

LANGMUIR

 

39 Yang, B; Lange-Jansen, H.C.; Scharnberg, M.; Wolfart, S.; Ludwig, K.; Adelung, R.; Kern, M.

"Influence of saliva contamination on zirconia ceramic bonding"

(2008) , 24 (4), pp. 508-513

DENTAL MATERIALS

 

38 Scharnberg, M; Adelung, R.; Faupel, F.

"Influence of top layer geometries on the electronic properties of pentacene and diindenoperylene thin films"

(2008) , 205 (3), pp. 578-590

PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE

 

37 Dora, SK; Bai, Y.X.; Elbahri, M.; Kunz, R.; Adelung, R.; Magnussen, O.

"Nanotunnel formation induced by Cu electrodeposition on 1T-TaS2"

(2008) , 155 (10), pp. D666-D670

JOURNAL OF THE ELECTROCHEMICAL SOCIETY

 

36 Yang, B; Wolfart, S.; Scharnberg, M.; Ludwig, K.; Adelung, R.; Kern, M.

"Influence of contamination on zirconia ceramic bonding"

(2007) , 86 (8), pp. 749-753

JOURNAL OF DENTAL RESEARCH

 

35 Elbahri, M; Paretkar, D.; Hirmas, K.; Jebril, S.; Adelung, R.

"Anti-Lotus effect for nanostructuring at the Leidenfrost temperature"

(2007) , 19 (9), pp. 1262-+

ADVANCED MATERIALS

 

34 Yang, B; Scharnberg, M.; Wolfart, S.; Quaas, A.C.; Ludwig, K.; Adelung, R.; Kern, M.

"Influence of contamination on bonding to zirconia ceramic"

(2007) , 81B (2), pp. 283-290

JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS

 

33 Hassel, AW; Milenkovic, S.; Schürmann, U.; Greve, H.; Zaporojtchenko, V.; Adelung, R.; Faupel, F.

"Model systems with extreme aspect ratio, tunable geometry, and surface functionality for a quantitative investigation of the lotus effect"

(2007) , 23 (4), pp. 2091-2094

LANGMUIR

 

32 Pannemann, C; Diekmann, T.; Hilleringmann, U.; Schürmann, U.; Scharnberg, M.; Zaporojtchenko, V.; Adelung, R.; Faupel, F.

"PTFE encapsulation for pentacene based organic thin film transistors"

(2007) , 25 (1), pp. 94-101

MATERIALS SCIENCE-POLAND

 

31 Scharnberg, M; Zaporojtchenko, V.; Adelung, R.; Faupel, F.; Pannemann, C.; Diekmann, T.; Hilleringmann, U.

"Tuning the threshold voltage of organic field-effect transistors by an electret encapsulating layer"

(2007) , 90 (1), Art.No. 013501

APPLIED PHYSICS LETTERS

 

30 Ramírez, C; Adelung, R.; Kipp, L.; Schattke, W.

"Adsorption and diffusion of an alkali-metal adatom on transition-metal dichalcogenides"

(2006) , 73 (19), Art.No. 195406

PHYSICAL REVIEW B

 

29 Elbahri, M; Rudra, S.K.; Wille, S.; Jebril, S.; Scharnberg, M.; Paretkar, D.; Kunz, R.; Rui, H.; Biswas, A.; Adelung, R.

"Employing thin-film delamination for the formation of shadow masks for nanostructure fabrication"

(2006) , 18 (8), pp. 1059-+

ADVANCED MATERIALS

 

28 Yang, B; Ludwig, K.; Adelung, R.; Kern, M.

"Micro-tensile bond strength of three luting resins to human regional dentin"

(2006) , 22 (1), pp. 45-56

DENTAL MATERIALS

 

27 Yang, B; Adelung, R.; Ludwig, K.; Bössmann, K.; Pashley, D.H.; Kern, M.

"Effect of structural change of collagen fibrils on the durability of dentin bonding"

(2005) , 26 (24), pp. 5021-5031

BIOMATERIALS

 

26 Scharnberg, M; Hu, J.; Kanzow, J.; Rätzke, K.; Adelung, R.; Faupel, F.; Pannemann, C.; Hilleringmann, U.; Meyer, S.; Pflaum, J.

"Radiotracer measurements as a sensitive tool for the detection of metal penetration in molecular-based organic electronics -: art. no. 024104"

(2005) , 86 (2), Art.No. 024104

APPLIED PHYSICS LETTERS

 

25 Ramírez, C; Adelung, R.; Kunz, R.; Kipp, L.; Schattke, W.

"Lithium adsorption by TiSe2 of varying concentration via density functional theory -: art. no. 035426"

(2005) , 71 (3), Art.No. 035426

PHYSICAL REVIEW B

 

24 Scharnberg, M; Hu, J.; Kanzow, J.; Rätzke, K.; Adelung, R.; Faupel, F.; Pflaum, J.

"Ag-diffusion in the organic semiconductor diindenoperyiene"

(2005) , 237-240, pp. 993-997

DIFFUSION IN MATERIALS: DIMAT 2004, PTS 1 AND 2

 

23 Biswas, A; Kunz, R.; Aktas, O.C.; Elbahri, M.; Adelung, R.; Takele, H.; Saeed, U.; Schürmann, U.; Zaporojtchenko, V.; Faupel, F.

"Arrays of wirelike microstructures of Ag with visible wavelength transparent plasmonic response at near-ultraviolet and midinfrared regions"

(2004) , 85 (11), pp. 1952-1954

APPLIED PHYSICS LETTERS

 

22 Morgenstern, M; Strasser, T.; Adelung, R.; Getzlaff, M.; Kipp, L.; Skibowski, M.; Schattke, W.; Wiesendanger, R.

"Contributions of the escape depth to the photoelectron intensity of a well-defined initial state"

(2004) , 70 (8), Art.No. 081305

PHYSICAL REVIEW B

 

21 Adelung, R; Ernst, F.; Zheng, N.; Landau, U.

"In situ nanoscale observation and control of electron-beam-induced cluster formation"

(2004) , 22 (4), pp. 1797-1802

JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B

 

20 Adelung, R; Aktas, O.C.; Franc, J.; Biswas, A.; Kunz, R.; Elbahri, M.; Kanzow, J.; Schürmann, U.; Faupel, F.

"Strain-controlled growth of nanowires within thin-film cracks"

(2004) , 3 (6), pp. 375-379

NATURE MATERIALS

 

19 Kreis, C; Werth, S.; Adelung, R.; Kipp, L.; Skibowski, M.; Krasovskii, E.E.; Schattke, W.

"Valence and conduction band states of HfS2:: From bulk to a single layer -: art. no. 235331"

(2003) , 68 (23), Art.No. 235331

PHYSICAL REVIEW B

 

18 Morgenstern, M; Klijn, J.; Meyer, C.; Getzlaff, M.; Johnson, R.L.; Adelung, R.; Kipp, L.; Römer, R.A.; Wiesendanger, R.

"Low density two-dimensional electron systems studied by scanning tunneling spectroscopy"

(2003) , 42 (7B), pp. 4809-4815

JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES &

 

17 Hollensteiner, S; Spiecker, E.; Dieker, C.; Jäger, W.; Adelung, R.; Kipp, L.; Skibowski, M.

"Self-assembled nanowire formation during Cu deposition on atomically flat Vse2 surfaces studied by microscopic methods"

(2003) , 23 (1-2), Art.No. PII S0928-4931(02)00264-3-179

MATERIALS SCIENCE & ENGINEERING C-BIOMIMETIC AND SUPRAMOLECULAR SYSTEMS

 

16 Adelung, R; Hartung, W.; Ernst, F.

"Fabrication of Cu-induced networks of linear nanostructures on different length scales"

(2002) , 50 (19), Art.No. PII S1359-6454(02)00370-1-4933

ACTA MATERIALIA

 

15 Morgenstern, M; Klijn, J.; Meyer, C.; Getzlaff, M.; Adelung, R.; Römer, R.A.; Rossnagel, K.; Kipp, L.; Skibowski, M.; Wiesendanger, R.

"Direct comparison between potential landscape and local density of states in a disordered two-dimensional electron system -: art. no. 136806"

(2002) , 89 (13), Art.No. 136806

PHYSICAL REVIEW LETTERS

 

14 Adelung, R; Ernst, F.; Scott, A.; Tabib-Azar, M.; Kipp, L.; Skibowski, M.; Hollensteiner, S.; Spiecker, E.; Jäger, W.; Gunst, S.; Klein, A.; Jägermann, W.; Zaporojtchenko, V.; Faupel, F.

"Self-assembled nanowire networks by deposition of copper onto layered-crystal surfaces"

(2002) , 14 (15), pp. 1056-+

ADVANCED MATERIALS

 

13 Kreis, C; Werth, S.; Adelung, R.; Kipp, L.; Skibowski, M.; Voss, D.; Krüger, P.; Mazur, A.; Pollmann, J.

"Surface resonances at transition metal dichalcogenide heterostructures -: art. no. 153314"

(2002) , 65 (15), Art.No. 153314

PHYSICAL REVIEW B

 

12 Kipp, L; Skibowski, M.; Johnson, R.L.; Berndt, R.; Adelung, R.; Harm, S.; Seemann, R.

"Sharper images by focusing soft X-rays with photon sieves"

(2001) , 414 (6860), pp. 184-188

NATURE

 

11 Adelung, R; Brandt, J.; Kipp, L.; Skibowski, M.

"Reconfiguration of charge density waves by surface nanostructures on TaS2 -: art. no. 165327"

(2001) , 63 (16), Art.No. 165327

PHYSICAL REVIEW B

 

10 Woedtke, S; Meeder, A.; Adelung, R.; Schwedhelm, R.; Kipp, L.; Skibowski, M.

"Structural properties of chlorinated epitaxial C60 films -: art. no. 155401"

(2001) , 63 (15), Art.No. 155401

PHYSICAL REVIEW B

 

9 Adelung, R; Brandt, J.; Rossnagel, K.; Seifarth, O.; Kipp, L.; Skibowski, P.; Ramírez, C.; Strasser, T.; Schattke, W.

"Tuning dimensionality by nanowire adsorption on layered materials"

(2001) , 86 (7), pp. 1303-1306

PHYSICAL REVIEW LETTERS

 

8 Kreis, C; Traving, M.; Adelung, R.; Kipp, L.; Skibowski, M.

"Tracing the valence band maximum during epitaxial growth of HfS2 on WSe2"

(2000) , 166 (1-4), pp. 17-22

APPLIED SURFACE SCIENCE

 

7 Kreis, C; Traving, M.; Adelung, R.; Kipp, L.; Skibowski, M.

"k-resolved electronic structure of quasi-free 2-dimensional HfS2 clusters"

(2000) , 52 (2), pp. 189-195

EUROPHYSICS LETTERS

 

6 Adelung, R; Brandt, J.; Tarcak, L.; Kipp, L.; Skibowski, M.

"Charge density waves affected by Rb nanowire network formation on 1T-TaS2"

(2000) , 162, pp. 666-669

APPLIED SURFACE SCIENCE

 

5 Starrost, F; Krasovskii, E.E.; Schattke, W.; Jockel, J.; Simon, U.; Adelung, R.; Kipp, L.

"Cetineites: Electronic, optical, and conduction properties of nanoporous chalcogenoantimonates"

(2000) , 61 (23), pp. 15697-15706

PHYSICAL REVIEW B

 

4 Adelung, R; Kipp, L.; Brandt, J.; Tarcak, L.; Traving, M.; Kreis, C.; Skibowski, M.

"Nanowire networks on perfectly flat surfaces"

(1999) , 74 (20), pp. 3053-3055

APPLIED PHYSICS LETTERS

 

3 Schwedhelm, R; Schlomka, J.P.; Woedtke, S.; Adelung, R.; Kipp, L.; Tolan, M.; Press, W.; Skibowski, M.

"Epitaxial thin-film growth of C60 on VSe2 studied with scanning tunneling microscopy and x-ray diffraction"

(1999) , 59 (20), pp. 13394-13400

PHYSICAL REVIEW B

 

2 Kipp, L; Adelung, R.; Wrobel, N.T.; Skibowski, M.

"Extrinsic surface states traced by surface photovoltage in photoemission"

(1999) , 74 (13), pp. 1836-1838

APPLIED PHYSICS LETTERS

 

1 Boehme, M; Adelung, R.; Traving, M.; Kipp, L.; Skibowski, M.

"Band bending, surface photovoltage and tunnelling microscopy on WSe2:Rb"

(1998) , 123, pp. 91-94

APPLIED SURFACE SCIENCE