2013
80. M. Baytekin, M.-D. Gerngross, Q. Li, S. Viebig, C. Selhuber-Unkel, J. Carstensen, H. Föll & R. Adelung
"Surface modification of Ti by chemical etching and HA sputtering for dental applications"
(2013) Proc. ICNBME 2, pp. 56
79. S. Bhowmick, D. Stauffer, H. Guo, S. Kaps, Y. K. Mishra, V. Hrkac, O. Warren, R. Adelung, A. Minor & L. Kienle
"In situ electromechanical study of ZnO nanowires"
(2013) Microscopy and Microanalysis Vol. 19(S2), pp. 434-435
78. L. Ghimpu, I. Tiginyanu, O. Lupan, Y. K. Mishra, I. Paulowicz, D. Gedamu, A. Cojocaru & R. Adelung
(2013) Vol. 1Semiconductor Conference (CAS), 2013 International, pp. 133-136
77. S. Hrkac, M. Abes, C. Koops, C. Krywka, M. Müller, S. Kaps, R. Adelung, J. McCord, E. Lage, E. Quandt, O. M. Magnussen & B. M. Murphy
"Local magnetization and strain in single magnetoelectric microrod composites"
(2013) Applied Physics Letters Vol. 103(12), pp. 123111
76. V. Hrkac, L. Kienle, S. Kaps, A. Lotnyk, Y. K. Mishra, U. Schurmann, V. Duppel, B. V. Lotsch & R. Adelung
"Superposition twinning supported by texture in ZnO nanospikes"
(2013) Journal of Applied Crystallography Vol. 46(2), pp. 396-403
75. X. Jin, M. Götz, S. Wille, Y. K. Mishra, R. Adelung & C. Zollfrank
(2013) Advanced Materials Vol. 25(9), pp. 1342-1347
74. H. Kaur, G. Pujari, A. Sarma, Y. K. Mishra, M. K. Jin, B. K. Nirala, N. K. Gohil, R. Adelung & D. K. Avasthi
"Study of in vitro toxicity of glucose capped gold nanoparticles in malignant and normal cell lines"
(2013) Advanced Materials Letters Vol. 4(12), pp. 888-894
73. Y. K. Mishra, S. Kaps, A. Schuchardt, I. Paulowicz, X. Jin, D. Gedamu, S. Freitag, M. Claus, S. Wille, A. Kovalev, S. N. Gorb & R. Adelung
(2013) Particle & Particle Systems Characterization Vol. 30(9), pp. 775-783
72. Y. Mishra, R. Adelung, G. Kumar, M. Elbahri, S. Mohapatra, R. Singhal, A. Tripathi & D. Avasthi
"Formation of self-organized silver nanocup-type structures and their plasmonic absorption"
(2013) Plasmonics Vol. 8(2), pp. 811-815
71. I. Tiginyanu, O. Volciuc, M. Stevens-Kalceff, V. Popa, J. Gutowski, S. Wille, R. Adelung & H. Föll
(2013) Surface Engineering and Applied Electrochemistry Vol. 49(1), pp. 1-3