Complete Wafer Process

First a schematic process flow graph is given for everything - from sand to wafer.
It includes side processes not covered in the backbone modules which, however, are self explanatory.
Si process flow
Next, we have a pictorial representation of just crystal growth and wafer production. Again, it contains some self-explanatory processes not introduced before.
From Poly-Si to the wafer

With frame With frame as PDF

go to 4.1.3 Silicon Crystal Growth and Wafer Production