Note: The “Lurtistn Sword” paged will be formatted somewhat differently (simpler) than the rest. As I grew older, my eyes deteriorated to a point where I can just barely type stuff in my html editor. I apologize for typos and perfectly spelled but wrong words produced by the erroe correction without me noticing.
My internal notes after buying the sword
 
Details
 
Severely corroded but about 1/3 of the blade is well preserved. One could make a case for seeing hints of a layered structure in this good part but that is not definite
. The workmanship of the very slender tip part of the blade is fabulous as is quite apparent even so almost 3000 years have passed.

No animal or heads on the hilt part.

Two rings of crimped construction

No decorations under pommel disc.

Some re-enforcement on the blade where it enters the hilt.

The pommel disc has a wide groove running through its diameter. That is a feature often found on IMAS swords. What it signifies is unclear. One might guess that is was supposed to act as a help to mount the heads but that is wrong. The heads are always mounted at right angle to this groove.
    
The pommel disc with big groove
     

With frame With frame as PDF

go to First Iron Swords - Provenance Problems

go to First Iron Swords - Bi-Metal Swords

go to First Iron Swords - Bi-Metal Swords

go to First Iron Swords - Double-Disc Hilt Sword

go to First Iron Swords - Large Pictures

go to First Iron Swords - First Iron Swords - Hallstatt Swords

go to Scythian Special Large Pictures

go to Luristan Special

go to First Iron Swords - Miscellaneous Objects

go to First Iron Swords - Places

go to First Iron Swords - Literature Digest

go to First Iron Swords - Luristan Type 1 Iron Swords

go to First Iron Swords - Luristan Type 2 Iron Swords

go to First Iron Swords - Bi-Metal Swords; Details

go to First Iron Swords - Luristan Type 1 Iron Swords

go to First Iron Swords - Reliefs / Sculptures with Swords and Daggers

© H. Föll (Iron, Steel and Swords script)