Large Pictures to "Lurisrtan Swords" |
 |
For some swords used in the Luristan project, large
scale pictures have been made which I will show here top preserve them for eternity. They are shown only ¼ of their
original size. You can restore the original size by copying the picture and inserting it into some image processor. |
| |
|
| | IMAS 8
or IR 3744 |
 |
Here are some high-resolution pictures of sworf IMAS 8
or IR 3744. This is the sword that we cut in half. More information about this sword can be found here and here. |
| |
|
|
|
|
| |
| |
IMAS 9 or IR 3743 |
 |
Here are some pictures of sworf IMAS 9
or IR 3743 More informatiomn in this link. |
| |
|
|
|
|
| |
| |
IMAS 10or IR 3745 |
 |
Here are some pictures of sworf IMAS 10or IR 3745
Note the unusual "banding" of the grip More information here |
| |
|
|
|
|
| |
| |
 |
Note the "banding" parttern at the grip part. |
| |
| |
|
|
| |
| |
| |
 |
This is a large-scale picture of the etched cross-section of the blade. Refer
to this link for details. 8ijn "project results". |
| |
| |
| |
IMAS 11or IR3746 |
 |
Here are some pictures of sworf IMAS 11or IR3746
Morer information here. |
| | |
|
|
| |
| |
v
With frame

Critical Museum Guide: Metropolitan Museum, NYC
Critical Museum Guide: Museums in Copenhagen
Critical Museum Guide: Landesmuseum Schleswig-Holstein in Schleswig, Germany
Israel Museum
Museums in Paris
Museums in the Balkan
Luristan Special
© H. Föll (Iron, Steel and Swords script)