Exercise 2.1-4

Derive the Formula for the Vacancy Equilibrium Concentration

Start from the formulas given, use the approximations described, and show that
cV   =  concentration
of vacancies
 =   SF
k 
 ·  exp – HF
kT
Would more advanced versions of Stirlings formula get better results?
 
 
 