| Note: The Lurtistn Sword paged will be formatted somewhat differently (simpler) than the rest. As I grew older, my eyes deteriorated to a point where I can just barely type stuff in my html editor. I apologize for typos and perfectly spelled but wrong words produced by the erroe correction without me noticing. | ||
| Her my personal notes after buying the swoerd | ||
| ||
| Note 2025: There is not much to add in hindsight. The sword still would be best used in for a (somewhat destructive) crystallographic analysis; possibly preceded by taking some x-rays. | ||
First Iron Swords - Provenance Problems
First Iron Swords - Bi-Metal Swords
First Iron Swords - Bi-Metal Swords
First Iron Swords - Double-Disc Hilt Sword
First Iron Swords - Large Pictures
First Iron Swords - First Iron Swords - Hallstatt Swords
Scythian Special Large Pictures
First Iron Swords - Miscellaneous Objects
First Iron Swords - Literature Digest
First Iron Swords - Luristan Type 1 Iron Swords
First Iron Swords - Luristan Type 2 Iron Swords
First Iron Swords - Bi-Metal Swords; Details
First Iron Swords - Luristan Type 1 Iron Swords
First Iron Swords - Reliefs / Sculptures with Swords and Daggers
© H. Föll (Iron, Steel and Swords script)