| A typical MOS transistor of 200x (x = 0 .... 5) vintage has a "gate length" (= distance between source an drain of about 0.5 µm and is run at about 3 V | ||
1.) What is the mobility the
material (= semiconductor) must have? Discuss the result for known mobility
values and consider the following points
|
||
2.) How could you increase
the speed for a given material
|
||
| Solution | ||
1.3.3 Ohms Law and Classical Physics
© H. Föll